Find suppliers for this alloyC80410
Chemical Composition
Element
Cu(1)
(1) Cu value includes Ag.
Min (%)99.9
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Rockwell F scale
As Centrifugal CastAs Centrifugal CastM0220   Min
25   Typ
6.5   Min
8   Typ
20   Min
25   Typ
30   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1981
Melting Point - Solidus°F1948
Densitylb/cu in. at 68°F0.323
Specific Gravity8.94
Electrical Conductivity% IACS at 68°F98
Coefficient of Thermal Expansion 68-39210⁻⁶ per °F (68 – 392°F)9.4
Modulus of Elasticity in Tensionksi17000
Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes
  • Casting
Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ElectricalElectrical ConductorsConductivity (Electrical)Electrical Conductivity
Electrical ConductorsConductivity (Thermal)Thermal Conductivity
Electrical ConductorsCorrosion ResistanceCorrosion Resistance
Electrical ConductorsCorrosion ResistanceOxidation Resistance
IndustrialCorrosion and Oxidation Resistant ApplicationsConductivity (Electrical)Electrical Conductivity
Corrosion and Oxidation Resistant ApplicationsConductivity (Thermal)Thermal Conductivity
Corrosion and Oxidation Resistant ApplicationsCorrosion ResistanceCorrosion Resistance
Corrosion and Oxidation Resistant ApplicationsCorrosion ResistanceOxidation Resistance
Rotor End RingsConductivity (Electrical)Electrical Conductivity
Rotor End RingsConductivity (Thermal)Thermal Conductivity
Rotor End RingsCorrosion ResistanceCorrosion Resistance
Rotor End RingsCorrosion ResistanceOxidation Resistance
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.