Find suppliers for this alloy
C81300
| Elements | |||
|---|---|---|---|
| Cu(1,2) | Be | Co | |
|
(1) Cu value includes Ag. (2) Cu + Sum of Named Elements 99.5% min. |
|||
| Min (%) | 98.5 | 0.02 | 0.6 |
| Max (%) | 0.10 | 1.0 | |
| Form | Temper | Temper Code | Brinell Hardness, 500 kg load |
|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||
| As Sand Cast | As Sand Cast | M01 | 89 Typ |
| Melting Point - Liquidus°F | 2000 |
|---|---|
| Melting Point - Solidus°F | 1950 |
| Densitylb/cu in. at 68°F | 0.318 |
| Specific Gravity | 8.81 |
| Electrical Conductivity% IACS at 68°F | 60 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 150 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 10 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.093 |
| Modulus of Elasticity in Tensionksi | 16000 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | Low |
| Drossing | Low |
| Effect of Section Size | Low |
| Fluidity | Medium |
| Gassing | High |
| Patternmakers Shrinkage inches per inch | 4/16 |
| Shrinkage in Solidification | High |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Fair |
| Machinability Rating | 20 |
Common Fabrication Processes
| Treatment | Minimum* | Maximum* | Value* | Time** | Medium |
|---|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | |||||
| Stress Relief | 500 | ||||
| Solution Treatment | 1800 | 1850 | 1 | Water | |
| Precipitation Treatment | 900 | 2 | Air | ||
Typical Uses
Applicable Specifications
Corrosion Properties