C81800
| Elements | ||||
|---|---|---|---|---|
| Cu(1) | Ag | Be | Co | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
||||
| Min (%) | 95.6 | 0.8 | 0.30 | 1.4 |
| Max (%) | 1.2 | 0.55 | 1.7 | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Rockwell B scale | Torsion Modulus (ksi) |
Proportional Limit (ksi) |
|---|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||||
| As Sand Cast | As Sand Cast | M01 |
50 Typ |
25 Typ |
20 Typ |
55 Typ |
6 Typ | 15 Typ |
| Precipitation Hardened | TF00 |
102 Typ |
75 Typ |
8 Typ |
96 Typ |
50 Typ | ||
| Melting Point - Liquidus°F | 1955 |
|---|---|
| Melting Point - Solidus°F | 1855 |
| Densitylb/cu in. at 68°F | 0.311 |
| Specific Gravity | 8.62 |
| Electrical Conductivity% IACS at 68°F | 45 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 150 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 10 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.1 |
| Modulus of Elasticity in Tensionksi | 16000 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | Low |
| Drossing | Low |
| Effect of Section Size | Low |
| Fluidity | Medium |
| Gassing | Medium |
| Patternmakers Shrinkage inches per inch | 3/16 |
| Shrinkage in Solidification | Medium |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Fair |
| Machinability Rating | 20 |
Common Fabrication Processes
| Treatment | Minimum* | Maximum* | Value* | Time** | Medium |
|---|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | |||||
| Stress Relief | 500 | ||||
| Solution Treatment | 1650 | 1700 | 1 | Water | |
| Precipitation Treatment | 900 | 3 | Air | ||