Chemical Composition
Element
Cu(1)PbSnZnFeNiAlBeCoCrSi
(1) Cu + Sum of Named Elements 99.5% min.
Min (%)1.901.00.20
Max (%)Rem0.020.100.100.250.200.152.151.20.090.35
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
As Sand CastPrecipitation HardenedTF00160   Min for Standard
150   Min for Standard
1   Min for Standard
Solution Heat TreatedTB0080   Min for Standard
45   Min for Standard
10   Min for Standard
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1800
Melting Point - Solidus°F1575
Densitylb/cu in. at 68°F0.298
Specific Gravity8.26
Electrical Conductivity% IACS at 68°F20
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F72.5
Coefficient of Thermal Expansion 68-39210⁻⁶ per °F (68 – 392°F)8.6
Specific Heat CapacityBtu/ lb /°F at 68°F0.1
Modulus of Elasticity in Tensionksi18500
Change in Density During Aging%0.6
Magnetic Permeability1.002
Poisson's Ratio0.3
Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes
  • Casting
Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
ArchitectureSculptureAppearanceAppearance
SculptureCasting CharacteristicsCastability
SculptureCorrosion ResistanceCorrosion Resistance
SculptureMechanical PropertiesVery High Strength
ConsumerGolf ClubsCorrosion ResistanceCorrosion Resistance
Golf ClubsMechanical PropertiesHigh Modulus of Elasticity
Golf ClubsMechanical PropertiesVery High Strength
JewelryAppearanceAppearance
JewelryCasting CharacteristicsCastability
JewelryCorrosion ResistanceCorrosion Resistance
JewelryMechanical PropertiesDuctility
JewelryMechanical PropertiesVery High Strength
Safety ToolsCorrosion ResistanceCorrosion Resistance
Safety ToolsMechanical PropertiesVery High Strength
Safety ToolsNon-MagneticNon-Magnetic
Safety ToolsNon-SparkingNon-Sparking
IndustrialAluminum Die Cast Plunger TipsConductivity (Thermal)Thermal Conductivity
Aluminum Die Cast Plunger TipsCorrosion ResistanceCorrosion Resistance
Aluminum Die Cast Plunger TipsMechanical PropertiesVery High Strength
Corrosion Resistant ValvesCorrosion ResistanceCorrosion Resistance
Corrosion Resistant ValvesCorrosion ResistanceCorrosion Resistance to Most Chemical Environments
Corrosion Resistant ValvesCorrosion ResistanceResists Stress Corrosion Cracking in Many Chemical Environments
Corrosion Resistant ValvesCorrosion ResistanceResists Stress Corrosion Cracking in Marine Environments
Corrosion Resistant ValvesFriction & Wear PropertiesExcellent Wear Resistance
Corrosion Resistant ValvesMechanical PropertiesVery High Strength
Glass MoldsConductivity (Thermal)Thermal Conductivity
Glass MoldsCorrosion ResistanceCorrosion Resistance
Glass MoldsFriction & Wear PropertiesWear Resistance
Glass MoldsMechanical PropertiesVery High Strength
Molds for Plastic PartsConductivity (Thermal)Thermal Conductivity
Molds for Plastic PartsCorrosion ResistanceCorrosion Resistance
Molds for Plastic PartsFriction & Wear PropertiesWear Resistance
Molds for Plastic PartsMechanical PropertiesVery High Strength
Permanent Molds for Brass and Aluminum CastingsConductivity (Thermal)Thermal Conductivity
Permanent Molds for Brass and Aluminum CastingsCorrosion ResistanceCorrosion Resistance
Permanent Molds for Brass and Aluminum CastingsFriction & Wear PropertiesWear Resistance
Permanent Molds for Brass and Aluminum CastingsMechanical PropertiesVery High Strength
MarineUndersea Cable HousingsConductivity (Electrical)Electrical Conductivity
Undersea Cable HousingsCorrosion ResistanceCorrosion Resistance
Undersea Cable HousingsCorrosion ResistanceCorrosion Resistance to Salt Water
Undersea Cable HousingsMechanical PropertiesVery High Strength
Applicable Specifications
Form Sub-Form System Standard Description
As Sand CastCastingsASTMB770COPPER-BERYLLIUM SAND CASTINGS
IngotASTMB30COPPER BASE ALLOYS IN INGOT FORM
Corrosion Properties

No information available.