C83300
| Elements | ||||
|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | |
|
(1) Cu + Sum of Named Elements 99.3% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. |
||||
| Min (%) | 92.0 | 1.0 | 1.0 | 2.0 |
| Max (%) | 94.0 | 2.0 | 2.0 | 6.0 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Rockwell B scale |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| As Sand Cast | As Sand Cast | M01 |
32 Typ |
10 Typ |
35 Typ |
35 Typ |
| Melting Point - Liquidus°F | 1940 |
|---|---|
| Melting Point - Solidus°F | 1886 |
| Densitylb/cu in. at 68°F | 0.318 |
| Specific Gravity | 8.8 |
| Electrical Conductivity% IACS at 68°F | 32 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 15000 |
Casting Characteristics
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Fair |
| Coated Metal Arc Welding | Not Recommended |
| Machinability Rating | 35 |
Common Fabrication Processes
| Treatment | Value* | Time** | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
| Stress Relief | 500 | |||
| Solution Treatment | 0 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Automotive | Battery Terminals | ||
| Electrical | Adaptors | Conductivity (Electrical) | Electrical Conductivity |
| Adaptors | Conductivity (Thermal) | Thermal Conductivity | |
| Adaptors | Corrosion Resistance | Corrosion Resistance | |
| Adaptors | Mechanical Properties | Moderate Strength | |
| Connectors | Conductivity (Electrical) | Electrical Conductivity | |
| Connectors | Conductivity (Thermal) | Thermal Conductivity | |
| Connectors | Corrosion Resistance | Corrosion Resistance | |
| Connectors | Mechanical Properties | Moderate Strength | |
| Electrical Components | Conductivity (Electrical) | Electrical Conductivity | |
| Electrical Components | Conductivity (Thermal) | Thermal Conductivity | |
| Electrical Components | Corrosion Resistance | Corrosion Resistance | |
| Electrical Components | Mechanical Properties | Moderate Strength | |
| Electrical Hardware Parts | Conductivity (Electrical) | Electrical Conductivity | |
| Electrical Hardware Parts | Conductivity (Thermal) | Thermal Conductivity | |
| Electrical Hardware Parts | Corrosion Resistance | Corrosion Resistance | |
| Electrical Hardware Parts | Mechanical Properties | Moderate Strength | |
| Terminal Ends for Electric Cables | Conductivity (Electrical) | Electrical Conductivity | |
| Terminal Ends for Electric Cables | Conductivity (Thermal) | Thermal Conductivity | |
| Terminal Ends for Electric Cables | Corrosion Resistance | Corrosion Resistance | |
| Terminal Ends for Electric Cables | Corrosion Resistance | Oxidation Resistance | |
| Terminal Ends for Electric Cables | Mechanical Properties | High Strength |
Applicable Specifications
Corrosion Properties