Find suppliers for this alloy
C83460
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P | Ni(3) | Al | S | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) Ni value includes Co. |
|||||||||||
| Min (%) | 2.5 | 4.0 | .50 | .05 | .15 | ||||||
| Max (%) | Rem | .09 | 4.5 | 6.0 | 1.0 | .10 | 1.0 | .005 | .6 | .25 | .005 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| As Sand Cast | As Sand Cast | M01 |
35.0 Typ |
16.0 Typ |
25 Typ |
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties