Find suppliers for this alloyC83460
Chemical Composition
Element
Cu(1,2)PbSnZnFePNi(3)AlSSbSi
(1) Cu + Sum of Named Elements 99.5% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) Ni value includes Co.
Min (%)2.54.0.50.05.15
Max (%)Rem.094.56.01.0.101.0.005.6.25.005
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
As Sand CastAs Sand CastM0135.0   Typ
16.0   Typ
25   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties

No physical properties for this alloy

Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.