Find suppliers for this alloy
C83500
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P(3) | Ni(4) | Al | S | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.3% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) For continuous castings P shall be 1.5% max. (4) Ni value includes Co. |
|||||||||||
| Min (%) | 86.0 | 3.5 | 5.5 | 1.0 | 0.50 | ||||||
| Max (%) | 88.0 | 5.5 | 6.5 | 2.5 | 0.25 | 0.03 | 1.0 | 0.005 | 0.08 | 0.25 | 0.005 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Builders Hardware | Door Hardware for Prisons | Appearance | Appearance |
| Door Hardware for Prisons | Corrosion Resistance | Corrosion Resistance | |
| Door Hardware for Prisons | Mechanical Properties | Moderate Strength | |
| Window Hardware | Appearance | Appearance | |
| Window Hardware | Corrosion Resistance | Corrosion Resistance | |
| Window Hardware | Mechanical Properties | Moderate Strength | |
| Consumer | Musical Instruments | Appearance | Appearance |
| Musical Instruments | Casting Characteristics | Castability | |
| Musical Instruments | Corrosion Resistance | Corrosion Resistance | |
| Musical Instruments | Damping Characteristics | Resonant Frequency, Damping Capacity | |
| Musical Instruments | Mechanical Properties | Moderate Strength | |
| Electrical | Electrical Equipment | Conductivity (Electrical) | Electrical Conductivity |
| Electrical Equipment | Conductivity (Thermal) | Thermal Conductivity | |
| Electrical Equipment | Corrosion Resistance | Corrosion Resistance | |
| Electrical Equipment | Mechanical Properties | Moderate Strength | |
| Marine | Marine Hardware | Corrosion Resistance | Corrosion Resistance |
| Marine Hardware | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Marine Hardware | Mechanical Properties | Moderate Strength |
Applicable Specifications
Corrosion Properties