Find suppliers for this alloyC83500
Chemical Composition
Element
Cu(1,2)PbSnZnFeP(3)Ni(4)AlSSbSi
(1) Cu + Sum of Named Elements 99.3% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) For continuous castings P shall be 1.5% max. (4) Ni value includes Co.
Min (%)86.03.55.51.00.50
Max (%)88.05.56.52.50.250.031.00.0050.080.250.005
Mechanical Properties

No mechanical properties for this alloy

Physical Properties

No physical properties for this alloy

Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes
  • Casting
Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
Builders HardwareDoor Hardware for PrisonsAppearanceAppearance
Door Hardware for PrisonsCorrosion ResistanceCorrosion Resistance
Door Hardware for PrisonsMechanical PropertiesModerate Strength
Window HardwareAppearanceAppearance
Window HardwareCorrosion ResistanceCorrosion Resistance
Window HardwareMechanical PropertiesModerate Strength
ConsumerMusical InstrumentsAppearanceAppearance
Musical InstrumentsCasting CharacteristicsCastability
Musical InstrumentsCorrosion ResistanceCorrosion Resistance
Musical InstrumentsDamping CharacteristicsResonant Frequency, Damping Capacity
Musical InstrumentsMechanical PropertiesModerate Strength
ElectricalElectrical EquipmentConductivity (Electrical)Electrical Conductivity
Electrical EquipmentConductivity (Thermal)Thermal Conductivity
Electrical EquipmentCorrosion ResistanceCorrosion Resistance
Electrical EquipmentMechanical PropertiesModerate Strength
MarineMarine HardwareCorrosion ResistanceCorrosion Resistance
Marine HardwareCorrosion ResistanceCorrosion Resistance to Salt Water
Marine HardwareMechanical PropertiesModerate Strength
Applicable Specifications
Form
Ingot
Corrosion Properties

No information available.