Find suppliers for this alloy
C83700
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu | Pb | Sn | Zn | Fe | P | Ni | Al | As | Mn | Si | |
| Min (%) | 83.0 | 0.05 | |||||||||
| Max (%) | 88.0 | 0.50 | 1.00 | Rem | 0.30 | 0.05 | 0.30 | 0.005 | 0.20 | 0.10 | 0.005 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties