Find suppliers for this alloy
C83810
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe(3) | Ni(4) | Al | Si | |
|
(1) Cu + Sum of Named Elements 99.3% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) Fe + Sb + As shall be 0.50% max. (4) Ni value includes Co. |
||||||||
| Min (%) | 4.0 | 2.0 | 7.5 | |||||
| Max (%) | Rem | 6.0 | 3.5 | 9.5 | 0.50 | 2.0 | 0.005 | 0.10 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties