Find suppliers for this alloyC84010
Chemical Composition
Element
Cu(1)PbSnZnFePNiAlBMnSSbSiZr
(1) Cu + Sum of Named Elements 99.3% min.
Min (%)82.02.05.00.500.010.10
Max (%)89.00.094.014.00.400.052.00.0050.100.200.650.020.0050.10
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Brinell Hardness, 500 kg load
CastingsAs Sand CastM0134.5   Min
38.5   Typ
15   Min
18   Typ
17   Min
30.5   Typ
65   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1895
Melting Point - Solidus°F1722
Densitylb/cu in. at 68°F0.309
Specific Gravity8.55
Electrical Conductivity% IACS at 68°F16
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F41.8
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)10
Specific Heat CapacityBtu/ lb /°F at 68°F0.094
Modulus of Elasticity in Tensionksi14700
Magnetic Permeability1
Casting Characteristics
Casting Attribute Level
Casting YieldHigh
DrossingMedium
Effect of Section SizeHigh
FluidityMedium
GassingMedium
Patternmakers Shrinkageinches per inch3/16
Shrinkage in SolidificationMedium
Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.