C84400
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P(3) | Ni(4) | Al | S | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.3% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) For continuous castings P shall be 1.5% max. (4) Ni value includes Co. |
|||||||||||
| Min (%) | 78.0 | 6.0 | 2.3 | 7.0 | |||||||
| Max (%) | 82.0 | 8.0 | 3.5 | 10.0 | 0.40 | 0.02 | 1.0 | 0.005 | 0.08 | 0.25 | 0.005 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load | Izod (ft-lbs) |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||||
| As Centrifugal Cast | As Centrifugal Cast | M02 |
29 Min for Standard |
13 Min for Standard |
18 Min for Standard |
||
| As Continuous Cast | As Continuous Cast | M07 |
30 Min for Standard |
15 Min for Standard |
16 Min for Standard |
||
| As Sand Cast | As Sand Cast | M01 |
29 Min for Standard 34 Typ |
13 Min for Standard 15 Typ |
18 Min for Standard 26 Typ |
55 Typ |
8 Typ |
| Melting Point - Liquidus°F | 1840 |
|---|---|
| Melting Point - Solidus°F | 1549 |
| Densitylb/cu in. at 68°F | 0.314 |
| Specific Gravity | 8.69 |
| Electrical Conductivity% IACS at 68°F | 16.4 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 41.8 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 10 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 13000 |
| Magnetic Permeability | 1 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | High |
| Drossing | Medium |
| Effect of Section Size | High |
| Fluidity | Medium |
| Gassing | Medium |
| Patternmakers Shrinkage inches per inch | 3/16 |
| Shrinkage in Solidification | Medium |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Not Recommended |
| Coated Metal Arc Welding | Fair |
| Machinability Rating | 90 |
Common Fabrication Processes
| Treatment | Value* | Time** | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
| Stress Relief | 500 | |||
| Solution Treatment | 0 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Architecture | Ornamental Fixtures | Appearance | Appearance |
| Ornamental Fixtures | Corrosion Resistance | Corrosion Resistance | |
| Ornamental Fixtures | Machining Properties | Machinability, Good | |
| Ornamental Fixtures | Mechanical Properties | Moderate Strength | |
| Builders Hardware | Cases for Dead Bolt Locks | Appearance | Appearance |
| Cases for Dead Bolt Locks | Corrosion Resistance | Corrosion Resistance | |
| Cases for Dead Bolt Locks | Machining Properties | Machinability, Good | |
| Cases for Dead Bolt Locks | Mechanical Properties | Moderate Strength | |
| Dead Bolt Locks | Appearance | Appearance | |
| Dead Bolt Locks | Corrosion Resistance | Corrosion Resistance | |
| Dead Bolt Locks | Machining Properties | Machinability, Good | |
| Dead Bolt Locks | Mechanical Properties | Moderate Strength | |
| Door Hardware for Prisons | Appearance | Appearance | |
| Door Hardware for Prisons | Casting Characteristics | Castability | |
| Door Hardware for Prisons | Corrosion Resistance | Corrosion Resistance | |
| Door Hardware for Prisons | Corrosion Resistance | Oxidation Resistance | |
| Door Hardware for Prisons | Machining Properties | Machinability, Good | |
| Door Hardware for Prisons | Mechanical Properties | Moderate Strength | |
| Hardware | Appearance | Appearance | |
| Hardware | Casting Characteristics | Castability | |
| Hardware | Corrosion Resistance | Corrosion Resistance | |
| Hardware | Corrosion Resistance | Oxidation Resistance | |
| Hardware | Machining Properties | Machinability, Good | |
| Hardware | Mechanical Properties | Moderate Strength | |
| Building | Cooling Equipment | Conductivity (Thermal) | Thermal Conductivity |
| Cooling Equipment | Corrosion Resistance | Corrosion Resistance | |
| Cooling Equipment | Mechanical Properties | Moderate Strength | |
| Heating Equipment | Conductivity (Thermal) | Thermal Conductivity | |
| Heating Equipment | Corrosion Resistance | Corrosion Resistance | |
| Heating Equipment | Mechanical Properties | Moderate Strength | |
| Consumer | Musical Instruments | Appearance | Appearance |
| Musical Instruments | Casting Characteristics | Castability | |
| Musical Instruments | Corrosion Resistance | Corrosion Resistance | |
| Musical Instruments | Damping Characteristics | Resonant Frequency, Damping Capacity | |
| Musical Instruments | Mechanical Properties | Moderate Strength | |
| Electrical | Electrical Equipment | Conductivity (Electrical) | Electrical Conductivity |
| Electrical Equipment | Conductivity (Thermal) | Thermal Conductivity | |
| Electrical Equipment | Corrosion Resistance | Corrosion Resistance | |
| Electrical Equipment | Corrosion Resistance | Oxidation Resistance | |
| Electrical Equipment | Mechanical Properties | Moderate Strength | |
| Industrial | Low Pressure Fittings | Corrosion Resistance | Corrosion Resistance |
| Low Pressure Fittings | Mechanical Properties | Moderate Strength | |
| Low Pressure Fittings | Pressure Tight | Pressure Tight | |
| Pump Fixtures | Corrosion Resistance | Corrosion Resistance | |
| Pump Fixtures | Friction & Wear Properties | Wear Resistance | |
| Pump Fixtures | Machining Properties | Machinability, Good | |
| Pump Fixtures | Mechanical Properties | Moderate Strength | |
| Valve Bodies for the Water Industry | Corrosion Resistance | Corrosion Resistance | |
| Valve Bodies for the Water Industry | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Valve Bodies for the Water Industry | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Valve Bodies for the Water Industry | Friction & Wear Properties | Wear Resistance | |
| Valve Bodies for the Water Industry | Machining Properties | Machinability, Good | |
| Valve Bodies for the Water Industry | Mechanical Properties | Moderate Strength | |
| Valve Seat | Corrosion Resistance | Corrosion Resistance | |
| Valve Seat | Friction & Wear Properties | Wear Resistance | |
| Valve Seat | Mechanical Properties | Moderate Strength | |
| Valves | Corrosion Resistance | Corrosion Resistance | |
| Valves | Friction & Wear Properties | Wear Resistance | |
| Valves | Machining Characteristics | Excellent Machinability | |
| Valves | Mechanical Properties | Moderate Strength | |
| Valves for Water Meters | Corrosion Resistance | Corrosion Resistance | |
| Valves for Water Meters | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Valves for Water Meters | Machining Properties | Machinability, Good | |
| Valves for Water Meters | Mechanical Properties | Moderate Strength | |
| Marine | Boat Parts | Appearance | Appearance |
| Boat Parts | Corrosion Resistance | Corrosion Resistance | |
| Boat Parts | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Boat Parts | Mechanical Properties | Moderate Strength | |
| Marine Hardware | Corrosion Resistance | Corrosion Resistance | |
| Marine Hardware | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Marine Hardware | Mechanical Properties | Moderate Strength | |
| Nuts for Transducers | Corrosion Resistance | Corrosion Resistance | |
| Nuts for Transducers | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Nuts for Transducers | Machining Properties | Machinability, Good | |
| Nuts for Transducers | Mechanical Properties | Moderate Strength | |
| Plumbing | Fixtures | Appearance | Appearance |
| Fixtures | Corrosion Resistance | Corrosion Resistance | |
| Fixtures | Machining Properties | Machinability, Good | |
| Fixtures | Mechanical Properties | Moderate Strength | |
| Fixtures | Pressure Tight | Pressure Tight | |
| Pipe Fittings | Corrosion Resistance | Corrosion Resistance | |
| Pipe Fittings | Mechanical Properties | Moderate Strength | |
| Pipe Fittings | Pressure Tight | Pressure Tight |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Centrifugal Cast | Castings | ASTM | B271/B271M | COPPER BASE ALLOY CENTRIFUGAL CASTINGS | |
| As Continuous Cast | Castings | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS | |
| As Sand Cast | Castings | ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS | |
| Castings | ASTM | B763/B763M | COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS | ||
| Fitting | ASME | B16.32 | CAST COPPER ALLOY SOLDER-JOINT FITTINGS FOR SOLVENT DRAINAGE SYSTEMS | ||
| ASME | B16.18 | CAST COPPER ALLOY SOLDER-JOINT PRESSURE FITTINGS | |||
| ASME | B16.24 | BRONZE PIPE FLANGES AND FLANGED FITTINGS | |||
| ASME | B16.23 | CAST COPPER ALLOY SOLDER-JOINT DRAINAGE FITTINGS - DWV | |||
| ASME | B16.15 | CAST BRONZE THREADED FITTINGS | |||
| ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS | |||
| ASME | B16.26 | CAST COPPER ALLOY FITTINGS FOR FLARED COPPER TUBES | |||
| Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM | ||
| Unions | FEDERAL | WW-U-516 | UNIONS, BRASS OR BRONZE |
Corrosion Properties