| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2,3) | Pb | Sn | Zn | Ni(4) | Al | Bi | Si | |
|
(1) In determining Cu min., Cu may be calculated as Cu + Ni. (2) Cu + Sum of Named Elements 99.3% min. (3) Fe + Sb + As shall be .8% max. (4) Ni value includes Co. |
||||||||
| Min (%) | 7.0 | 3.0 | 7.0 | |||||
| Max (%) | Rem | 9.0 | 4.5 | 11.0 | 1.0 | 0.01 | 0.05 | 0.2 |