Find suppliers for this alloy
C85210
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni | Al | As | Si | |
|
(1) Cu + Sum of Named Elements 98.9% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. |
|||||||||
| Min (%) | 70.0 | 2.0 | 1.0 | 0.02 | |||||
| Max (%) | 75.0 | 5.0 | 3.0 | Rem | 0.8 | 1.0 | 0.005 | 0.06 | 0.005 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties