Find suppliers for this alloy C85563
Chemical Composition
Elements
Cu(1) Pb Sn Zn Fe Ni Al As Mn
(1) Cu + Sum of Named Elements 99.5% min.
Min (%) 61.5 0.20 0.50 0.04
Max (%) 63.5 1.6 0.30 Rem 0.30 0.20 0.7 0.14 0.10
Mechanical Properties *
Form Temper Temper Code Tensile Strength
(ksi)
YS-0.2% Offset
(ksi)
Elongation
(%)
Brinell Hardness, 3000 kg load
* Measured at room temperature, 68°F (20°C).
As Permanent Mold Cast M05 40.6 Min
16.0 Min
10 Typ
70 Min
Physical Properties

No physical properties for this alloy

Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties

No fabrication properties for this alloy

Common Fabrication Processes

No fabrication process properties for this alloy

Typical Uses

No information for this alloy

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties