Find suppliers for this alloy
C85566
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | Ni | Al | As | Mn | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||||||||||
| Min (%) | 62.0 | 0.45 | 0.02 | 0.02 | |||||||
| Max (%) | 65.0 | 0.20 | 0.30 | Rem | 0.20 | 0.20 | 0.7 | 0.04 | 0.10 | 0.05 | 0.02 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Typical Uses
Applicable Specifications
Corrosion Properties