Find suppliers for this alloy
C85600
| Elements | ||||||
|---|---|---|---|---|---|---|
| Cu | Pb | Sn | Zn | Ni | Mn | |
| Min (%) | 59.0 | |||||
| Max (%) | 63.0 | 0.20 | 0.20 | Rem | 0.20 | 0.20 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties