Find suppliers for this alloy
C85690
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | P | Al | B | Cr | Mn | Se | |
|
(1) Cu + Sum of Named Elements 99.8% min. |
||||||||||
| Min (%) | 62.5 | 0.30 | 0.03 | 0.02 | 0.001 | 0.03 | 0.03 | 0.05 | ||
| Max (%) | 65.0 | 0.10 | 0.9 | Rem | 0.09 | 0.06 | 0.003 | 0.09 | 0.09 | 0.15 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Shear Strength (ksi) |
Compressive Yield Strength (ksi) |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||||
| Rod | As Permanent Mold Cast | M05 |
53.5 Typ |
20.3 Typ |
50 Typ |
39.9 Typ |
166.4 Typ |
| Melting Point - Liquidus°F | 1702 |
|---|---|
| Melting Point - Solidus°F | 1636 |
| Densitylb/cu in. at 68°F | 0.304 |
| Specific Gravity | 8.43 |
| Electrical Conductivity% IACS at 68°F | 24.3 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 49.8 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 11.5 |
| Modulus of Elasticity in Tensionksi | 10430 |
| Poisson's Ratio | 0.409 |
Casting Characteristics
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Forgeability Rating | 95 |
| Machinability Rating | 85 |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties