Find suppliers for this alloy
C85705
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni | Al | Mn | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||||||||||
| Min (%) | 58.0 | 1.8 | 0.50 | 0.50 | 0.04 | ||||||
| Max (%) | 60.0 | 2.5 | 0.8 | Rem | 0.8 | 0.02 | 1.2 | 0.8 | 0.20 | 0.05 | 0.05 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Brinell Hardness, 3000 kg load |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| As Permanent Mold Cast | M05 |
43.5 Min |
21.8 Min |
15 Min |
90 Min |
|
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Typical Uses
Applicable Specifications
Corrosion Properties