C85710
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu | Pb | Sn | Zn | Fe | Ni | Al | Mn | Si | |
| Min (%) | 58.0 | 1.0 | 0.20 | ||||||
| Max (%) | 63.0 | 2.5 | 1.0 | Rem | 0.8 | 1.0 | 0.8 | 0.50 | 0.05 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
Elongation (%) |
|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||
| As Sand Cast | As Sand Cast | M01 |
50 Min for Standard |
25 Min for Standard |