Find suppliers for this alloyC85710
Chemical Composition
Element
CuPbSnZnFeNiAlMnSi
Min (%)58.01.00.20
Max (%)63.02.51.0Rem0.81.00.80.500.05
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
As Sand CastAs Sand CastM0150   Min for Standard
20   Min for Standard
25   Min for Standard
* Measured at room temperature, 68°F (20°C).
Physical Properties

No physical properties for this alloy

Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.