C85910
| Elements | ||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni | Al | B | Mn | S | Sb | Si | Zr | |
|
(1) Cu + Sum of Named Elements 99.3% min. |
||||||||||||||
| Min (%) | 58.0 | 31.0 | 0.10 | 0.01 | 0.10 | |||||||||
| Max (%) | 62.0 | 0.09 | 1.5 | 41.0 | 0.50 | 0.01 | 1.5 | 0.6 | 0.20 | 0.20 | 0.65 | 0.20 | 0.25 | 0.20 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Castings | As Sand Cast | M01 |
56 Min 60 Typ |
23 Min 26 Typ |
20 Min 28 Typ |
85 Typ |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.101 |
|---|---|
| Modulus of Elasticity in Tensionksi | 15600 |