Find suppliers for this alloyC85910
Chemical Composition
Element
Cu(1)PbSnZnFePNiAlBMnSSbSiZr
(1) Cu + Sum of Named Elements 99.3% min.
Min (%)58.031.00.100.010.10
Max (%)62.00.091.541.00.500.011.50.60.200.200.650.200.250.20
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Brinell Hardness, 500 kg load
CastingsAs Sand CastM0156   Min
60   Typ
23   Min
26   Typ
20   Min
28   Typ
85   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Specific Heat CapacityBtu/ lb /°F at 68°F0.101
Modulus of Elasticity in Tensionksi15600
Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties

No fabrication properties for this alloy

Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical Uses

No information available.

Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.