Chemical Composition
Element
Cu(1,2)PbSnZnFeNi(3)AlMn
(1) Cu + Sum of Named Elements 99.0% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) Ni value includes Co.
Min (%)60.022.02.05.02.5
Max (%)66.00.200.2028.04.01.07.55.0
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
YS-0.5% Ext
(ksi)
Elongation
(%)
Brinell Hardness, 3000 kg load
Izod
(ft-lbs)
Charpy V-Notch Impact Strength
(ft-lbs)
Compression Deformation Limit
(ksi)
Compressive Strength .001 in. set/in.
(ksi)
Compressive Strength .1 in. set/in.
(ksi)
Creep Strength (0.1% per 10,000 hours)
(ksi)
Fatigue Strength**
(ksi)
As Centrifugal CastAs Centrifugal CastM02110   Min for Standard
83   Typ
65   Typ
12   Min for Standard
As Continuous CastAs Continuous CastM07110   Min for Standard
62   Min for Standard
14   Min for Standard
As Sand CastAs Sand CastM01110   Min for Standard
119   Typ
60   Min for Standard
62   Typ
12   Min for Standard
18   Typ
223   Min for Standard
225   Typ
15   Typ
12   Typ
55   Min for Standard
60   Typ
97   Typ
19   Typ
25   Typ
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106.
Physical Properties
(1) Field Strength 16 kA/m
Melting Point - Liquidus°F1693
Melting Point - Solidus°F1625
Densitylb/cu in. at 68°F0.283
Specific Gravity7.83
Electrical Conductivity% IACS at 68°F8
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F20.5
Coefficient of Thermal Expansion 68-57210⁻⁶ per °F (68 – 572°F)12
Specific Heat CapacityBtu/ lb /°F at 68°F0.09
Modulus of Elasticity in Tensionksi14200
Magnetic Permeability1.09(1)
Casting Characteristics
Casting Attribute Level
Casting YieldLow
DrossingHigh
Effect of Section SizeLow
FluidityMedium
GassingLow
Patternmakers Shrinkageinches per inch4/16
Shrinkage in SolidificationHigh
Fabrication Properties
Technique Suitability
SolderingPoor
BrazingPoor
Oxyacetylene WeldingPoor
Gas Shielded Arc WeldingPoor
Coated Metal Arc WeldingGood
Machinability Rating8
Common Fabrication Processes
  • Casting
    
Thermal Properties
Treatment Value* Time**
* Temperature is measured in Fahrenheit. ** Time is measured in minutes.
Stress Relief500
Solution Treatment0
Typical uses
Product Category Product Reason Category Reason
Builders HardwareBracketsCorrosion ResistanceCorrosion Resistance
BracketsFriction & Wear PropertiesWear Resistance
BracketsMechanical PropertiesHigh Strength
ElectricalElectrical ComponentsConductivity (Electrical)Electrical Conductivity
Electrical ComponentsConductivity (Thermal)Thermal Conductivity
Electrical ComponentsCorrosion ResistanceCorrosion Resistance
Electrical ComponentsMechanical PropertiesHigh Strength
SwitchesConductivity (Electrical)Electrical Conductivity
SwitchesConductivity (Thermal)Thermal Conductivity
SwitchesCorrosion ResistanceCorrosion Resistance
SwitchesMechanical PropertiesHigh Strength
FastenersScrew Down NutsCorrosion ResistanceCorrosion Resistance
Screw Down NutsCorrosion ResistanceCorrosion Resistance
Screw Down NutsMechanical PropertiesHigh Strength
Screw Down NutsMechanical PropertiesHigh Strength
IndustrialBridge PinsCorrosion ResistanceCorrosion Resistance
Bridge PinsFriction & Wear PropertiesWear Resistance
Bridge PinsMechanical PropertiesHigh Strength
BushingsCorrosion ResistanceCorrosion Resistance
BushingsFriction & Wear PropertiesWear Resistance
BushingsMechanical PropertiesHigh Strength
CamsCorrosion ResistanceCorrosion Resistance
CamsFriction & Wear PropertiesWear Resistance
CamsMechanical PropertiesHigh Strength
Forming Dies for Wood Pulp IndustryCorrosion ResistanceCorrosion Resistance
Forming Dies for Wood Pulp IndustryFriction & Wear PropertiesWear Resistance
Forming Dies for Wood Pulp IndustryMechanical PropertiesHigh Strength
FramesCorrosion ResistanceCorrosion Resistance
FramesMechanical PropertiesHigh Strength
GearsCorrosion ResistanceCorrosion Resistance
GearsFriction & Wear PropertiesWear Resistance
GearsMechanical PropertiesHigh Strength
GibCorrosion ResistanceCorrosion Resistance
GibFriction & Wear PropertiesWear Resistance
GibMechanical PropertiesHigh Strength
High Strength Machine PartsConductivity (Thermal)Thermal Conductivity
High Strength Machine PartsCorrosion ResistanceCorrosion Resistance
High Strength Machine PartsFriction & Wear PropertiesWear Resistance
High Strength Machine PartsMechanical PropertiesHigh Strength
HooksCorrosion ResistanceCorrosion Resistance
HooksMechanical PropertiesHigh Strength
Hydraulic Cylinder PartsCorrosion ResistanceCorrosion Resistance
Hydraulic Cylinder PartsFriction & Wear PropertiesWear Resistance
Hydraulic Cylinder PartsMechanical PropertiesHigh Strength
Large Valve StemsCorrosion ResistanceCorrosion Resistance
Large Valve StemsFriction & Wear PropertiesWear Resistance
Large Valve StemsMechanical PropertiesHigh Strength
PropellersCorrosion ResistanceCorrosion Resistance
PropellersFriction & Wear PropertiesWear Resistance
PropellersMechanical PropertiesHigh Strength
Slow Speed, Heavy Load BearingsCorrosion ResistanceCorrosion Resistance
Slow Speed, Heavy Load BearingsFriction & Wear PropertiesWear Resistance
Slow Speed, Heavy Load BearingsMechanical PropertiesHigh Strength
StrutsCorrosion ResistanceCorrosion Resistance
StrutsMechanical PropertiesHigh Strength
Wear Rings for Forming Dies for Wood Pulp IndustryCorrosion ResistanceCorrosion Resistance
Wear Rings for Forming Dies for Wood Pulp IndustryFriction & Wear PropertiesWear Resistance
Wear Rings for Forming Dies for Wood Pulp IndustryMechanical PropertiesHigh Strength
MarineBoat PartsCorrosion ResistanceCorrosion Resistance
Boat PartsCorrosion ResistanceCorrosion Resistance to Salt Water
Boat PartsFriction & Wear PropertiesWear Resistance
Boat PartsMechanical PropertiesHigh Strength
ClampsCorrosion ResistanceCorrosion Resistance
ClampsCorrosion ResistanceCorrosion Resistance to Salt Water
ClampsFriction & Wear PropertiesWear Resistance
ClampsMechanical PropertiesHigh Strength
Covers for Marine HardwareAppearanceAppearance
Covers for Marine HardwareCorrosion ResistanceCorrosion Resistance
Covers for Marine HardwareCorrosion ResistanceCorrosion Resistance to Salt Water
Covers for Marine HardwareFriction & Wear PropertiesWear Resistance
Covers for Marine HardwareMechanical PropertiesHigh Strength
Marine HardwareAppearanceAppearance
Marine HardwareCorrosion ResistanceCorrosion Resistance
Marine HardwareCorrosion ResistanceCorrosion Resistance to Salt Water
Marine HardwareMechanical PropertiesHigh Strength
RuddersCorrosion ResistanceCorrosion Resistance
RuddersCorrosion ResistanceCorrosion Resistance to Salt Water
RuddersFriction & Wear PropertiesWear Resistance
RuddersMechanical PropertiesHigh Strength
Applicable Specifications
Form Sub-Form System Standard Description
As Centrifugal CastCastingsAMS4862MANGANESE BRONZE CASTINGS, SAND AND CENTRIFUGAL, HIGH STRENGTH, AS CAST
CastingsASTMB271/B271MCOPPER BASE ALLOY CENTRIFUGAL CASTINGS
CastingsSAEJ461WROUGHT AND CAST COPPER ALLOYS
CastingsSAEJ462CAST COPPER ALLOYS
As Continuous CastCastingsASTMB505/B505MCOPPER BASE ALLOY CONTINUOUS CASTINGS
As Sand CastCastingsAMS4862MANGANESE BRONZE CASTINGS, SAND AND CENTRIFUGAL, HIGH STRENGTH, AS CAST
CastingsASTMB22/B22MBRONZE CASTINGS FOR BRIDGES AND TURNTABLES
CastingsASTMB584COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS
CastingsASTMB763/B763MCOPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS
CastingsSAEJ461WROUGHT AND CAST COPPER ALLOYS
CastingsSAEJ462CAST COPPER ALLOYS
Ingot
ASTMB30COPPER BASE ALLOYS IN INGOT FORM
FEDERALQQ-C-523COPPER ALLOY INGOTS: BRASS (YELLOW HIGH STRENGTH) MANGANESE AND MANGANESE-ALUMINUM BRONZE
Precision CastCastingsMILITARYMIL-C-11866CASTINGS, PRECISION, NONFERROUS
Valves
Corrosion Properties

No information available.