Find suppliers for this alloy
C86400
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Al | Mn | |
|
(1) Cu + Sum of Named Elements 99.0% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) Ni value includes Co. |
||||||||
| Min (%) | 56.0 | 0.50 | 0.50 | 34.0 | 0.40 | 0.50 | 0.10 | |
| Max (%) | 62.0 | 1.5 | 1.5 | 42.0 | 2.0 | 1.0 | 1.5 | 1.5 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load | Brinell Hardness, 3000 kg load | Izod (ft-lbs) |
Charpy V-Notch Impact Strength (ft-lbs) |
Compressive Strength .001 in. set/in. (ksi) |
Compressive Strength .1 in. set/in. (ksi) |
Fatigue Strength** (ksi) |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106. | ||||||||||||
| As Centrifugal Cast | As Centrifugal Cast | M02 |
60 Min for Standard |
20 Min for Standard |
15 Min for Standard |
|||||||
| As Sand Cast | As Sand Cast | M01 |
60 Min for Standard 65 Typ |
20 Min for Standard 25 Typ |
15 Min for Standard 20 Typ |
90 Typ |
105 Typ |
30 Typ | 25 Typ |
22 Typ | 87 Typ | 25 Typ |
| Melting Point - Liquidus°F | 1616 |
|---|---|
| Melting Point - Solidus°F | 1583 |
| Densitylb/cu in. at 68°F | 0.301 |
| Specific Gravity | 8.33 |
| Electrical Conductivity% IACS at 68°F | 19 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 51 |
| Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 11 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 14000 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | Low |
| Drossing | High |
| Effect of Section Size | Low |
| Fluidity | Medium |
| Gassing | Low |
| Patternmakers Shrinkage inches per inch | 4/16 |
| Shrinkage in Solidification | High |
| Technique | Suitability |
|---|---|
| Soldering | Fair |
| Brazing | Fair |
| Oxyacetylene Welding | Poor |
| Gas Shielded Arc Welding | Poor |
| Coated Metal Arc Welding | Poor |
| Machinability Rating | 65 |
Common Fabrication Processes
| Treatment | Value* | Time** | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
| Stress Relief | 500 | |||
| Solution Treatment | 0 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Builders Hardware | Door hardware for Prison | Appearance | Appearance |
| Door hardware for Prison | Corrosion Resistance | Corrosion Resistance | |
| Door hardware for Prison | Machining Characteristics | Excellent Machinability (Free Machining) | |
| Door hardware for Prison | Mechanical Properties | High Strength | |
| Window Hardware | Appearance | Appearance | |
| Window Hardware | Corrosion Resistance | Corrosion Resistance | |
| Window Hardware | Machining Characteristics | Excellent Machinability (Free Machining) | |
| Window Hardware | Mechanical Properties | High Strength | |
| Consumer | Musical Instruments | Appearance | Appearance |
| Musical Instruments | Corrosion Resistance | Corrosion Resistance | |
| Musical Instruments | Damping Characteristics | Resonant Frequency, Damping Capacity | |
| Musical Instruments | Friction & Wear Properties | Wear Resistance | |
| Musical Instruments | Machining Characteristics | Excellent Machinability (Free Machining) | |
| Musical Instruments | Mechanical Properties | High Strength | |
| Piano Keys | Appearance | Appearance | |
| Piano Keys | Corrosion Resistance | Corrosion Resistance | |
| Piano Keys | Friction & Wear Properties | Wear Resistance | |
| Piano Keys | Mechanical Properties | High Strength | |
| Electrical | Electrical Components | Conductivity (Electrical) | Electrical Conductivity |
| Electrical Components | Conductivity (Thermal) | Thermal Conductivity | |
| Electrical Components | Corrosion Resistance | Corrosion Resistance | |
| Electrical Components | Mechanical Properties | High Strength | |
| Electrical Equipment | Conductivity (Electrical) | Electrical Conductivity | |
| Electrical Equipment | Conductivity (Thermal) | Thermal Conductivity | |
| Electrical Equipment | Corrosion Resistance | Corrosion Resistance | |
| Electrical Equipment | Mechanical Properties | High Strength | |
| Switches | Conductivity (Electrical) | Electrical Conductivity | |
| Switches | Conductivity (Thermal) | Thermal Conductivity | |
| Switches | Corrosion Resistance | Corrosion Resistance | |
| Switches | Mechanical Properties | High Strength | |
| Fasteners | Screw Down Nuts | Corrosion Resistance | Corrosion Resistance |
| Screw Down Nuts | Friction & Wear Properties | Wear Resistance | |
| Screw Down Nuts | Mechanical Properties | High Strength | |
| Screw Down Nuts | Mechanical Properties | Moderate Strength | |
| Industrial | Bearing Cage Blanks | Corrosion Resistance | Corrosion Resistance |
| Bearing Cage Blanks | Friction & Wear Properties | Wear Resistance | |
| Bearing Cage Blanks | Mechanical Properties | High Strength | |
| Bearings | Corrosion Resistance | Corrosion Resistance | |
| Bearings | Friction & Wear Properties | Wear Resistance | |
| Bearings | Machining Properties | Machinability, Good | |
| Bearings | Mechanical Properties | High Strength | |
| Brackets | Corrosion Resistance | Corrosion Resistance | |
| Brackets | Friction & Wear Properties | Wear Resistance | |
| Brackets | Machining Characteristics | Excellent Machinability | |
| Brackets | Mechanical Properties | High Strength | |
| Bushings | Corrosion Resistance | Corrosion Resistance | |
| Bushings | Friction & Wear Properties | Wear Resistance | |
| Bushings | Mechanical Properties | High Strength | |
| Cams | Corrosion Resistance | Corrosion Resistance | |
| Cams | Friction & Wear Properties | Wear Resistance | |
| Cams | Machining Characteristics | Excellent Machinability | |
| Cams | Mechanical Properties | High Strength | |
| Fittings | Corrosion Resistance | Corrosion Resistance | |
| Fittings | Friction & Wear Properties | Wear Resistance | |
| Fittings | Machining Characteristics | Excellent Machinability | |
| Fittings | Mechanical Properties | High Strength | |
| Lever Arms | Corrosion Resistance | Corrosion Resistance | |
| Lever Arms | Friction & Wear Properties | Wear Resistance | |
| Lever Arms | Mechanical Properties | High Strength | |
| Light Duty Gears | Corrosion Resistance | Corrosion Resistance | |
| Light Duty Gears | Friction & Wear Properties | Wear Resistance | |
| Light Duty Gears | Machining Properties | Machinability, Good | |
| Light Duty Gears | Mechanical Properties | High Strength | |
| Machinery Parts | Corrosion Resistance | Corrosion Resistance | |
| Machinery Parts | Friction & Wear Properties | Wear Resistance | |
| Machinery Parts | Machining Characteristics | Excellent Machinability | |
| Machinery Parts | Mechanical Properties | High Strength | |
| Propellers | Corrosion Resistance | Corrosion Resistance | |
| Propellers | Friction & Wear Properties | Wear Resistance | |
| Propellers | Mechanical Properties | High Strength | |
| Pump Fixtures | Corrosion Resistance | Corrosion Resistance | |
| Pump Fixtures | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Pump Fixtures | Machining Properties | Machinability, Good | |
| Pump Fixtures | Mechanical Properties | Moderate Strength | |
| Roller Bearings | Corrosion Resistance | Corrosion Resistance | |
| Roller Bearings | Friction & Wear Properties | Wear Resistance | |
| Roller Bearings | Mechanical Properties | High Strength | |
| Valve Stems | Corrosion Resistance | Corrosion Resistance | |
| Valve Stems | Mechanical Properties | Ductility | |
| Valve Stems | Mechanical Properties | High Strength | |
| Marine | Boat Parts | Corrosion Resistance | Corrosion Resistance |
| Boat Parts | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Boat Parts | Friction & Wear Properties | Wear Resistance | |
| Boat Parts | Mechanical Properties | High Strength | |
| Covers for Marine Hardware | Appearance | Appearance | |
| Covers for Marine Hardware | Corrosion Resistance | Corrosion Resistance | |
| Covers for Marine Hardware | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Covers for Marine Hardware | Mechanical Properties | High Strength | |
| Marine Fittings | Corrosion Resistance | Corrosion Resistance | |
| Marine Fittings | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Marine Fittings | Friction & Wear Properties | Wear Resistance | |
| Marine Fittings | Machining Characteristics | Excellent Machinability (Free Machining) | |
| Marine Fittings | Mechanical Properties | High Strength | |
| Marine Hardware | Appearance | Appearance | |
| Marine Hardware | Corrosion Resistance | Corrosion Resistance | |
| Marine Hardware | Corrosion Resistance | Corrosion Resistance to Salt Water | |
| Marine Hardware | Machining Characteristics | Excellent Machinability | |
| Marine Hardware | Mechanical Properties | High Strength | |
| Plumbing | Fixtures | Appearance | Appearance |
| Fixtures | Corrosion Resistance | Corrosion Resistance | |
| Fixtures | Friction & Wear Properties | Wear Resistance | |
| Fixtures | Machining Characteristics | Excellent Machinability (Free Machining) | |
| Fixtures | Mechanical Properties | High Strength |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Centrifugal Cast | Castings | ASTM | B271/B271M | COPPER BASE ALLOY CENTRIFUGAL CASTINGS | |
| As Sand Cast | Castings | ASTM | B763/B763M | COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS | |
| Castings | ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS | ||
| Ingot | FEDERAL | QQ-C-523 | COPPER ALLOY INGOTS: BRASS (YELLOW HIGH STRENGTH) MANGANESE AND MANGANESE-ALUMINUM BRONZE | ||
| ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM | |||
| Valves |
Corrosion Properties