Find suppliers for this alloy
C87440
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||||||||
| Min (%) | 81.0 | 11.0 | 0.50 | ||||||
| Max (%) | 0.09 | 0.20 | 16.0 | 0.20 | 0.15 | 0.10 | 0.10 | 2.0 | |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties