Find suppliers for this alloyC87600
Element | ||||||
---|---|---|---|---|---|---|
Cu(1) | Pb | Zn | Fe | Mn | Si | |
(1) Cu + Sum of Named Elements 99.5% min. | ||||||
Min (%) | 88.0 | 4.0 | 3.5 | |||
Max (%) | 0.09 | 7.0 | 0.20 | 0.25 | 5.5 |
Form | Temper | Temper Code | Tensile Strength (ksi) | YS-0.5% Ext (ksi) | Elongation (%) | Rockwell B scale | Brinell Hardness, 500 kg load | Brinell Hardness, 3000 kg load | Compressive Strength .1 in. set/in. (ksi) | ||
---|---|---|---|---|---|---|---|---|---|---|---|
As Centrifugal Cast | As Centrifugal Cast | M02 | 60 Min for Standard | 30 Min for Standard | 16 Min for Standard | ||||||
As Sand Cast | As Sand Cast | M01 | 60 Min for Standard 66 Typ | 30 Min for Standard 32 Typ | 16 Min for Standard 20 Typ | 76 Typ | 110 Typ | 135 Typ | 60 Typ | ||
* Measured at room temperature, 68°F (20°C). |
Melting Point - Liquidus°F | 1780 |
---|---|
Melting Point - Solidus°F | 1580 |
Densitylb/cu in. at 68°F | 0.3 |
Specific Gravity | 8.3 |
Electrical Conductivity% IACS at 68°F | 6 |
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 16.4 |
Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
Modulus of Elasticity in Tensionksi | 17000 |
Casting Attribute | Level |
---|---|
Casting Yield | Medium |
Drossing | Low |
Effect of Section Size | Medium |
Fluidity | High |
Gassing | High |
Patternmakers Shrinkageinches per inch | 3/16 |
Shrinkage in Solidification | Medium |
Technique | Suitability |
---|---|
Soldering | Excellent |
Brazing | Excellent |
Oxyacetylene Welding | Fair |
Gas Shielded Arc Welding | Excellent |
Coated Metal Arc Welding | Good |
Spot Weld | Good |
Seam Weld | Good |
Butt Weld | Good |
Machinability Rating | 40 |
Common Fabrication Processes
- Casting
Treatment | Value* | Time** | |||
---|---|---|---|---|---|
* Temperature is measured in Fahrenheit. ** Time is measured in minutes. | |||||
Stress Relief | 500 | ||||
Solution Treatment | 0 |
Product Category | Product | Reason Category | Reason |
---|---|---|---|
Architecture | Artistry Components | Appearance | Appearance |
Artistry Components | Casting Characteristics | Castability | |
Artistry Components | Corrosion Resistance | Corrosion Resistance | |
Artistry Components | Mechanical Properties | High Strength | |
Electrical | Electrical Components | Casting Characteristics | Castability |
Electrical Components | Conductivity (Electrical) | Electrical Conductivity | |
Electrical Components | Conductivity (Thermal) | Thermal Conductivity | |
Electrical Components | Corrosion Resistance | Corrosion Resistance | |
Electrical Components | Mechanical Properties | High Strength | |
Industrial | Bearings | Casting Characteristics | Castability |
Bearings | Corrosion Resistance | Corrosion Resistance | |
Bearings | Mechanical Properties | High Strength | |
Engineering Applications | Casting Characteristics | Castability | |
Engineering Applications | Corrosion Resistance | Corrosion Resistance | |
Engineering Applications | Mechanical Properties | High Strength | |
Valve Bodies | Casting Characteristics | Castability | |
Valve Bodies | Corrosion Resistance | Corrosion Resistance | |
Valve Bodies | Mechanical Properties | High Strength | |
Valve Stems | Corrosion Resistance | Corrosion Resistance | |
Valve Stems | Mechanical Properties | Ductility | |
Valve Stems | Mechanical Properties | High Strength |
Form | Sub-Form | System | Standard | Description |
---|---|---|---|---|
As Centrifugal Cast | ASTM | B271/B271M | COPPER BASE ALLOY CENTRIFUGAL CASTINGS | |
As Sand Cast | Castings | ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS |
Castings | ASTM | B763/B763M | COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS | |
Ingot | ||||
ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties