Find suppliers for this alloy
C87860
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Mn | Si | Zr | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
||||||||||
| Min (%) | 75.0 | .05 | 2.7 | .002 | ||||||
| Max (%) | 79.0 | .09 | .30 | Rem | .10 | .20 | .20 | .10 | 3.5 | .030 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Rockwell B scale |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| As Sand Cast | As Sand Cast | M01 |
55.1 Min 65.3 Typ |
20.3 Min 26.1 Typ |
15 Min |
60 Typ |
| Permanent Mold Castings | As Permanent Mold Cast | M05 |
62.4 Min 72.5 Typ |
23.2 Min 29 Typ |
15 Min |
65 Typ |
| Melting Point - Liquidus°F | 1643 |
|---|---|
| Melting Point - Solidus°F | 1571 |
| Densitylb/cu in. at 68°F | 0.3 |
| Specific Gravity | 8.3 |
| Electrical Conductivity% IACS at 68°F | 8 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 21.7 |
| Coefficient of Thermal Expansion 68-21210 to -6 power per °F (68 – 212°F) | 10.3 |
| Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 10.3 |
| Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) | 10.4 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 15200 |
| Poisson's Ratio | 0.33 |
Casting Characteristics
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Good |
| Gas Shielded Arc Welding | Good |
| Coated Metal Arc Welding | Good |
| Spot Weld | Good |
| Seam Weld | Good |
| Butt Weld | Good |
| Capacity for Being Cold Worked | Poor |
| Capacity for Being Hot Formed | Excellent |
| Forgeability Rating | 95 |
| Machinability Rating | 70 |
Common Fabrication Processes
| Treatment | Minimum* | Maximum* | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. | ||||
| Annealing | 932 | 1112 | ||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Industrial | Bolts | ||
| Nuts | |||
| Plumbing | Lead-free defined as Calif. AB 1953 max. .25% lead content | ||
| Potable Water Components, Valves, Pump Components , Plumbing Fittings, Meter Cases |
Applicable Specifications
Corrosion Properties