| Elements | |||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu | Pb | Sn | Zn | Fe | P | Ni | Al | As | Mn | S | Sb | Si | |
| Min (%) | 63.0 | 30.0 | 0.8 | ||||||||||
| Max (%) | 0.25 | 0.25 | 36.0 | 0.40 | 0.01 | 0.50 | 0.15 | 0.05 | 0.15 | 0.05 | 0.05 | 1.2 | |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Rockwell B scale | Charpy V-Notch Impact Strength (ft-lbs) |
|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||||
| As Die Cast | As Pressure Die Cast | M04 |
70 Typ 70 Typ |
35 Typ |
25 Typ 25 Typ |
70 Typ |
50 Typ 50 Typ |
| Melting Point - Liquidus°F | 1700 |
|---|---|
| Melting Point - Solidus°F | 1650 |
| Densitylb/cu in. at 68°F | 0.308 |
| Specific Gravity | 8.5 |
| Electrical Conductivity% IACS at 68°F | 15 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 15000 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | High |
| Drossing | High |
| Effect of Section Size | Medium |
| Fluidity | Medium |
| Gassing | Low |
| Patternmakers Shrinkage inches per inch | 3/16 |
| Shrinkage in Solidification | Medium |
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Not Recommended |
| Coated Metal Arc Welding | Not Recommended |
| Machinability Rating | 80 |
Common Fabrication Processes
| Treatment | Value* | Time** | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
| Stress Relief | 500 | |||
| Solution Treatment | 0 | |||