C87950
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | P | Al | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||||||
| Min (%) | 58.0 | 0.30 | 0.10 | 0.30 | |||
| Max (%) | 65.0 | 0.09 | 1.5 | Rem | 0.15 | 0.8 | 1.5 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| Strip | As Sand Cast | M01 |
45 Min 50 Typ 55 Max |
25 Min 30 Typ 35 Max |
4 Min |
| Melting Point - Liquidus°F | 1598 |
|---|---|
| Melting Point - Solidus°F | 1580 |
| Densitylb/cu in. at 68°F | 0.3 |
| Specific Gravity | 8.33 |
| Electrical Conductivity% IACS at 68°F | 14 |
Casting Characteristics
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Good |
| Gas Shielded Arc Welding | Good |
| Coated Metal Arc Welding | Good |
| Capacity for Being Cold Worked | Poor |
| Capacity for Being Hot Formed | Excellent |
| Forgeability Rating | 95 |
| Machinability Rating | 80 |