Find suppliers for this alloy
C89320
| Elements | ||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Al | Bi | S | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
||||||||||||
| Min (%) | 87.0 | 5.0 | 4.0 | |||||||||
| Max (%) | 91.0 | 0.09 | 7.0 | 1.0 | 0.20 | 0.30 | 1.0 | 0.005 | 6.0 | 0.08 | 0.35 | 0.005 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Brinell Hardness, 500 kg load | Charpy V-Notch Impact Strength (ft-lbs) |
Compressive Strength .01 in. set/in. (ksi) |
|---|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||||
| As Centrifugal Cast | As Centrifugal Cast | M02 |
35 Min 40 Typ |
18 Min 20 Typ |
15 Min 30 Typ |
70 Typ |
14 Typ |
20 Typ |
| As Continuous Cast | As Continuous Cast | M07 |
35 Min for Standard 40 Typ |
18 Min for Standard 20 Typ |
15 Min for Standard 30 Typ |
70 Typ |
14 Typ |
20 Typ |
| As Permanent Mold Cast | As Permanent Mold Cast | M05 |
35 Min 40 Typ |
18 Min 20 Typ |
15 Min 30 Typ |
70 Typ |
14 Typ |
20 Typ |
| Melting Point - Liquidus°F | 1913 |
|---|---|
| Melting Point - Solidus°F | 1702 |
| Densitylb/cu in. at 68°F | 0.318 |
| Specific Gravity | 8.8 |
| Electrical Conductivity% IACS at 68°F | 14.7 |
| Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F | 32.4 |
| Modulus of Elasticity in Tensionksi | 13900 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | High |
| Drossing | Low |
| Effect of Section Size | Medium |
| Fluidity | Medium |
| Gassing | Medium |
| Shrinkage in Solidification | Low |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Not Recommended |
| Coated Metal Arc Welding | Not Recommended |
| Machinability Rating | 80 |
Common Fabrication Processes
| Treatment | Time** | |||
|---|---|---|---|---|
| ** Time is measured in minutes. | ||||
| Solution Treatment | 0 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Fasteners | Washers | Corrosion Resistance | Corrosion Resistance |
| Washers | Lead Free | Lead Free | |
| Washers | Machining Properties | Machinability, Good | |
| Washers | Mechanical Properties | Moderate Strength | |
| Industrial | Backs for Lined Bearings | Corrosion Resistance | Corrosion Resistance |
| Backs for Lined Bearings | Friction & Wear Properties | Wear Resistance | |
| Backs for Lined Bearings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Backs for Lined Bearings | Machining Properties | Machinability, Good | |
| Cam Bushings for Diesel Engines | Corrosion Resistance | Corrosion Resistance | |
| Cam Bushings for Diesel Engines | Friction & Wear Properties | Wear Resistance | |
| Cam Bushings for Diesel Engines | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Cam Bushings for Diesel Engines | Machining Properties | Machinability, Good | |
| Crankshaft Main Bearings | Corrosion Resistance | Corrosion Resistance | |
| Crankshaft Main Bearings | Friction & Wear Properties | Anti-Seizing Properties | |
| Crankshaft Main Bearings | Friction & Wear Properties | Low Coefficient of Friction | |
| Crankshaft Main Bearings | Friction & Wear Properties | Wear Resistance | |
| Crankshaft Main Bearings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Crankshaft Main Bearings | Machining Properties | Machinability, Good | |
| Deep Well Pump Bowl Bushings | Corrosion Resistance | Corrosion Resistance | |
| Deep Well Pump Bowl Bushings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Deep Well Pump Bowl Bushings | Friction & Wear Properties | Wear Resistance | |
| Deep Well Pump Bowl Bushings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Deep Well Pump Bowl Bushings | Machining Properties | Machinability, Good | |
| Deep Well Pump Line Shaft Bearings | Corrosion Resistance | Corrosion Resistance | |
| Deep Well Pump Line Shaft Bearings | Corrosion Resistance | Corrosion Resistance to Many Industrial Chemicals | |
| Deep Well Pump Line Shaft Bearings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Deep Well Pump Line Shaft Bearings | Friction & Wear Properties | Wear Resistance | |
| Deep Well Pump Line Shaft Bearings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Deep Well Pump Line Shaft Bearings | Machining Properties | Machinability, Good | |
| Electric Motor Bearings | Corrosion Resistance | Corrosion Resistance | |
| Electric Motor Bearings | Friction & Wear Properties | Anti-Seizing Properties | |
| Electric Motor Bearings | Friction & Wear Properties | Low Coefficient of Friction | |
| Electric Motor Bearings | Friction & Wear Properties | Wear Resistance | |
| Electric Motor Bearings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Electric Motor Bearings | Machining Properties | Machinability, Good | |
| General Utility Bearings | Corrosion Resistance | Corrosion Resistance | |
| General Utility Bearings | Lead Free | Lead Free | |
| General Utility Bearings | Machining Properties | Machinability, Good | |
| General Utility Bearings | Mechanical Properties | Moderate Strength | |
| General Utility Bushings | Corrosion Resistance | Corrosion Resistance | |
| General Utility Bushings | Lead Free | Lead Free | |
| General Utility Bushings | Machining Properties | Machinability, Good | |
| General Utility Bushings | Mechanical Properties | Moderate Strength | |
| Guide Bushings for Piston Rods | Corrosion Resistance | Corrosion Resistance | |
| Guide Bushings for Piston Rods | Friction & Wear Properties | Anti-Seizing Properties | |
| Guide Bushings for Piston Rods | Friction & Wear Properties | Low Coefficient of Friction | |
| Guide Bushings for Piston Rods | Friction & Wear Properties | Wear Resistance | |
| Guide Bushings for Piston Rods | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Guide Bushings for Piston Rods | Machining Properties | Machinability, Good | |
| Guide Bushings for Valves | Corrosion Resistance | Corrosion Resistance | |
| Guide Bushings for Valves | Friction & Wear Properties | Anti-Seizing Properties | |
| Guide Bushings for Valves | Friction & Wear Properties | Low Coefficient of Friction | |
| Guide Bushings for Valves | Friction & Wear Properties | Wear Resistance | |
| Guide Bushings for Valves | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Guide Bushings for Valves | Machining Properties | Machinability, Good | |
| Hydraulic Gland Seals | Corrosion Resistance | Corrosion Resistance | |
| Hydraulic Gland Seals | Friction & Wear Properties | Anti-Seizing Properties | |
| Hydraulic Gland Seals | Friction & Wear Properties | Low Coefficient of Friction | |
| Hydraulic Gland Seals | Friction & Wear Properties | Wear Resistance | |
| Hydraulic Gland Seals | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Hydraulic Gland Seals | Machining Properties | Machinability, Good | |
| Main Bearings for Presses | Corrosion Resistance | Corrosion Resistance | |
| Main Bearings for Presses | Friction & Wear Properties | Anti-Seizing Properties | |
| Main Bearings for Presses | Friction & Wear Properties | Low Coefficient of Friction | |
| Main Bearings for Presses | Friction & Wear Properties | Wear Resistance | |
| Main Bearings for Presses | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Main Bearings for Presses | Machining Properties | Machinability, Good | |
| Piston Pin Bearings | Corrosion Resistance | Corrosion Resistance | |
| Piston Pin Bearings | Friction & Wear Properties | Anti-Seizing Properties | |
| Piston Pin Bearings | Friction & Wear Properties | Low Coefficient of Friction | |
| Piston Pin Bearings | Friction & Wear Properties | Wear Resistance | |
| Piston Pin Bearings | Lead-Free | Lead-Free Alternative to Leaded Alloy | |
| Piston Pin Bearings | Machining Properties | Machinability, Good | |
| Pump Sleeves | Corrosion Resistance | Corrosion Resistance | |
| Pump Sleeves | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Pump Sleeves | Friction & Wear Properties | Wear Resistance | |
| Pump Sleeves | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Rod Bushings | Corrosion Resistance | Corrosion Resistance | |
| Rod Bushings | Friction & Wear Properties | Anti-Seizing Properties | |
| Rod Bushings | Friction & Wear Properties | Low Coefficient of Friction | |
| Rod Bushings | Friction & Wear Properties | Wear Resistance | |
| Rod Bushings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Rod Bushings | Machining Properties | Machinability, Good | |
| Rolling Mill Bearings | Corrosion Resistance | Corrosion Resistance | |
| Rolling Mill Bearings | Friction & Wear Properties | Anti-Seizing Properties | |
| Rolling Mill Bearings | Friction & Wear Properties | Low Coefficient of Friction | |
| Rolling Mill Bearings | Friction & Wear Properties | Wear Resistance | |
| Rolling Mill Bearings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Rolling Mill Bearings | Machining Properties | Machinability, Good | |
| Seals | Corrosion Resistance | Corrosion Resistance | |
| Seals | Friction & Wear Properties | Anti-Seizing Properties | |
| Seals | Friction & Wear Properties | Low Coefficient of Friction | |
| Seals | Friction & Wear Properties | Wear Resistance | |
| Seals | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Seals | Machining Properties | Machinability, Good | |
| Sleeve Bushings (for cranes, etc.) | Corrosion Resistance | Corrosion Resistance | |
| Sleeve Bushings (for cranes, etc.) | Friction & Wear Properties | Anti-Seizing Properties | |
| Sleeve Bushings (for cranes, etc.) | Friction & Wear Properties | Low Coefficient of Friction | |
| Sleeve Bushings (for cranes, etc.) | Friction & Wear Properties | Wear Resistance | |
| Sleeve Bushings (for cranes, etc.) | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Sleeve Bushings (for cranes, etc.) | Machining Properties | Machinability, Good | |
| Spacer Bushings (for Pumps, etc.) | Corrosion Resistance | Corrosion Resistance | |
| Spacer Bushings (for Pumps, etc.) | Friction & Wear Properties | Anti-Seizing Properties | |
| Spacer Bushings (for Pumps, etc.) | Friction & Wear Properties | Low Coefficient of Friction | |
| Spacer Bushings (for Pumps, etc.) | Friction & Wear Properties | Wear Resistance | |
| Spacer Bushings (for Pumps, etc.) | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Spacer Bushings (for Pumps, etc.) | Machining Properties | Machinability, Good | |
| Wrist Pin Bushings | Corrosion Resistance | Corrosion Resistance | |
| Wrist Pin Bushings | Friction & Wear Properties | Anti-Seizing Properties | |
| Wrist Pin Bushings | Friction & Wear Properties | Low Coefficient of Friction | |
| Wrist Pin Bushings | Friction & Wear Properties | Wear Resistance | |
| Wrist Pin Bushings | Lead Free | Lead-Free Alternative to Leaded Alloy | |
| Wrist Pin Bushings | Machining Properties | Machinability, Good |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Continuous Cast | ASTM | B505/B505M | COPPER BASE ALLOY CONTINUOUS CASTINGS | ||
| Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties