Find suppliers for this alloyC89320
Chemical Composition
Element
Cu(1)PbSnZnFePNi(2)AlBiSSbSi
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co.
Min (%)87.05.04.0
Max (%)91.00.097.01.00.200.301.00.0056.00.080.350.005
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Brinell Hardness, 500 kg load
Charpy V-Notch Impact Strength
(ft-lbs)
Compressive Strength .01 in. set/in.
(ksi)
As Centrifugal CastAs Centrifugal CastM0235   Min
40   Typ
18   Min
20   Typ
15   Min
30   Typ
70   Typ
14   Typ
20   Typ
As Continuous CastAs Continuous CastM0735   Min for Standard
40   Typ
18   Min for Standard
20   Typ
15   Min for Standard
30   Typ
70   Typ
14   Typ
20   Typ
As Permanent Mold CastAs Permanent Mold CastM0535   Min
40   Typ
18   Min
20   Typ
15   Min
30   Typ
70   Typ
14   Typ
20   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1913
Melting Point - Solidus°F1702
Densitylb/cu in. at 68°F0.318
Specific Gravity8.8
Electrical Conductivity% IACS at 68°F14.7
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F32.4
Modulus of Elasticity in Tensionksi13900
Casting Characteristics
Casting Attribute Level
Casting YieldHigh
DrossingLow
Effect of Section SizeMedium
FluidityMedium
GassingMedium
Shrinkage in SolidificationLow
Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingGood
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingNot Recommended
Coated Metal Arc WeldingNot Recommended
Machinability Rating80
Common Fabrication Processes
  • Casting
    
Thermal Properties
Treatment Time**
* Temperature is measured in Fahrenheit. ** Time is measured in minutes.
Solution Treatment0
Typical uses
Product Category Product Reason Category Reason
FastenersWashersCorrosion ResistanceCorrosion Resistance
WashersLead FreeLead Free
WashersMachining PropertiesMachinability, Good
WashersMechanical PropertiesModerate Strength
IndustrialBacks for Lined BearingsCorrosion ResistanceCorrosion Resistance
Backs for Lined BearingsFriction & Wear PropertiesWear Resistance
Backs for Lined BearingsLead FreeLead-Free Alternative to Leaded Alloy
Backs for Lined BearingsMachining PropertiesMachinability, Good
Cam Bushings for Diesel EnginesCorrosion ResistanceCorrosion Resistance
Cam Bushings for Diesel EnginesFriction & Wear PropertiesWear Resistance
Cam Bushings for Diesel EnginesLead FreeLead-Free Alternative to Leaded Alloy
Cam Bushings for Diesel EnginesMachining PropertiesMachinability, Good
Crankshaft Main BearingsCorrosion ResistanceCorrosion Resistance
Crankshaft Main BearingsFriction & Wear PropertiesAnti-Seizing Properties
Crankshaft Main BearingsFriction & Wear PropertiesLow Coefficient of Friction
Crankshaft Main BearingsFriction & Wear PropertiesWear Resistance
Crankshaft Main BearingsLead FreeLead-Free Alternative to Leaded Alloy
Crankshaft Main BearingsMachining PropertiesMachinability, Good
Deep Well Pump Bowl BushingsCorrosion ResistanceCorrosion Resistance
Deep Well Pump Bowl BushingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Deep Well Pump Bowl BushingsFriction & Wear PropertiesWear Resistance
Deep Well Pump Bowl BushingsLead FreeLead-Free Alternative to Leaded Alloy
Deep Well Pump Bowl BushingsMachining PropertiesMachinability, Good
Deep Well Pump Line Shaft BearingsCorrosion ResistanceCorrosion Resistance
Deep Well Pump Line Shaft BearingsCorrosion ResistanceCorrosion Resistance to Many Industrial Chemicals
Deep Well Pump Line Shaft BearingsCorrosion ResistanceCorrosion Resistance to Numerous Environments
Deep Well Pump Line Shaft BearingsFriction & Wear PropertiesWear Resistance
Deep Well Pump Line Shaft BearingsLead FreeLead-Free Alternative to Leaded Alloy
Deep Well Pump Line Shaft BearingsMachining PropertiesMachinability, Good
Electric Motor BearingsCorrosion ResistanceCorrosion Resistance
Electric Motor BearingsFriction & Wear PropertiesAnti-Seizing Properties
Electric Motor BearingsFriction & Wear PropertiesLow Coefficient of Friction
Electric Motor BearingsFriction & Wear PropertiesWear Resistance
Electric Motor BearingsLead FreeLead-Free Alternative to Leaded Alloy
Electric Motor BearingsMachining PropertiesMachinability, Good
General Utility BearingsCorrosion ResistanceCorrosion Resistance
General Utility BearingsLead FreeLead Free
General Utility BearingsMachining PropertiesMachinability, Good
General Utility BearingsMechanical PropertiesModerate Strength
General Utility BushingsCorrosion ResistanceCorrosion Resistance
General Utility BushingsLead FreeLead Free
General Utility BushingsMachining PropertiesMachinability, Good
General Utility BushingsMechanical PropertiesModerate Strength
Guide Bushings for Piston RodsCorrosion ResistanceCorrosion Resistance
Guide Bushings for Piston RodsFriction & Wear PropertiesAnti-Seizing Properties
Guide Bushings for Piston RodsFriction & Wear PropertiesLow Coefficient of Friction
Guide Bushings for Piston RodsFriction & Wear PropertiesWear Resistance
Guide Bushings for Piston RodsLead FreeLead-Free Alternative to Leaded Alloy
Guide Bushings for Piston RodsMachining PropertiesMachinability, Good
Guide Bushings for ValvesCorrosion ResistanceCorrosion Resistance
Guide Bushings for ValvesFriction & Wear PropertiesAnti-Seizing Properties
Guide Bushings for ValvesFriction & Wear PropertiesLow Coefficient of Friction
Guide Bushings for ValvesFriction & Wear PropertiesWear Resistance
Guide Bushings for ValvesLead FreeLead-Free Alternative to Leaded Alloy
Guide Bushings for ValvesMachining PropertiesMachinability, Good
Hydraulic Gland SealsCorrosion ResistanceCorrosion Resistance
Hydraulic Gland SealsFriction & Wear PropertiesAnti-Seizing Properties
Hydraulic Gland SealsFriction & Wear PropertiesLow Coefficient of Friction
Hydraulic Gland SealsFriction & Wear PropertiesWear Resistance
Hydraulic Gland SealsLead FreeLead-Free Alternative to Leaded Alloy
Hydraulic Gland SealsMachining PropertiesMachinability, Good
Main Bearings for PressesCorrosion ResistanceCorrosion Resistance
Main Bearings for PressesFriction & Wear PropertiesAnti-Seizing Properties
Main Bearings for PressesFriction & Wear PropertiesLow Coefficient of Friction
Main Bearings for PressesFriction & Wear PropertiesWear Resistance
Main Bearings for PressesLead FreeLead-Free Alternative to Leaded Alloy
Main Bearings for PressesMachining PropertiesMachinability, Good
Piston Pin BearingsCorrosion ResistanceCorrosion Resistance
Piston Pin BearingsFriction & Wear PropertiesAnti-Seizing Properties
Piston Pin BearingsFriction & Wear PropertiesLow Coefficient of Friction
Piston Pin BearingsFriction & Wear PropertiesWear Resistance
Piston Pin BearingsLead-FreeLead-Free Alternative to Leaded Alloy
Piston Pin BearingsMachining PropertiesMachinability, Good
Pump SleevesCorrosion ResistanceCorrosion Resistance
Pump SleevesCorrosion ResistanceCorrosion Resistance to Numerous Environments
Pump SleevesFriction & Wear PropertiesWear Resistance
Pump SleevesLead FreeLead-Free Alternative to Leaded Alloy
Rod BushingsCorrosion ResistanceCorrosion Resistance
Rod BushingsFriction & Wear PropertiesAnti-Seizing Properties
Rod BushingsFriction & Wear PropertiesLow Coefficient of Friction
Rod BushingsFriction & Wear PropertiesWear Resistance
Rod BushingsLead FreeLead-Free Alternative to Leaded Alloy
Rod BushingsMachining PropertiesMachinability, Good
Rolling Mill BearingsCorrosion ResistanceCorrosion Resistance
Rolling Mill BearingsFriction & Wear PropertiesAnti-Seizing Properties
Rolling Mill BearingsFriction & Wear PropertiesLow Coefficient of Friction
Rolling Mill BearingsFriction & Wear PropertiesWear Resistance
Rolling Mill BearingsLead FreeLead-Free Alternative to Leaded Alloy
Rolling Mill BearingsMachining PropertiesMachinability, Good
SealsCorrosion ResistanceCorrosion Resistance
SealsFriction & Wear PropertiesAnti-Seizing Properties
SealsFriction & Wear PropertiesLow Coefficient of Friction
SealsFriction & Wear PropertiesWear Resistance
SealsLead FreeLead-Free Alternative to Leaded Alloy
SealsMachining PropertiesMachinability, Good
Sleeve Bushings (for cranes, etc.)Corrosion ResistanceCorrosion Resistance
Sleeve Bushings (for cranes, etc.)Friction & Wear PropertiesAnti-Seizing Properties
Sleeve Bushings (for cranes, etc.)Friction & Wear PropertiesLow Coefficient of Friction
Sleeve Bushings (for cranes, etc.)Friction & Wear PropertiesWear Resistance
Sleeve Bushings (for cranes, etc.)Lead FreeLead-Free Alternative to Leaded Alloy
Sleeve Bushings (for cranes, etc.)Machining PropertiesMachinability, Good
Spacer Bushings (for Pumps, etc.)Corrosion ResistanceCorrosion Resistance
Spacer Bushings (for Pumps, etc.)Friction & Wear PropertiesAnti-Seizing Properties
Spacer Bushings (for Pumps, etc.)Friction & Wear PropertiesLow Coefficient of Friction
Spacer Bushings (for Pumps, etc.)Friction & Wear PropertiesWear Resistance
Spacer Bushings (for Pumps, etc.)Lead FreeLead-Free Alternative to Leaded Alloy
Spacer Bushings (for Pumps, etc.)Machining PropertiesMachinability, Good
Wrist Pin BushingsCorrosion ResistanceCorrosion Resistance
Wrist Pin BushingsFriction & Wear PropertiesAnti-Seizing Properties
Wrist Pin BushingsFriction & Wear PropertiesLow Coefficient of Friction
Wrist Pin BushingsFriction & Wear PropertiesWear Resistance
Wrist Pin BushingsLead FreeLead-Free Alternative to Leaded Alloy
Wrist Pin BushingsMachining PropertiesMachinability, Good
Applicable Specifications
Form System Standard Description
As Continuous CastASTMB505/B505MCOPPER BASE ALLOY CONTINUOUS CASTINGS
IngotASTMB30COPPER BASE ALLOYS IN INGOT FORM
Corrosion Properties