Find suppliers for this alloyC89530
Chemical Composition
Element
Cu(1)PbSnZnFePNi(2)AlBiSbSiSe
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co.
Min (%)84.03.57.01.00.10
Max (%)89.00.206.09.00.300.051.00.012.00.200.010.30
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Brinell Hardness, 3000 kg load
Shear Strength
(ksi)
Impact Strength
(ksi)
Compressive Yield Strength
(ksi)
Fatigue Strength**
(ksi)
As Sand CastAs Sand CastM0128.3   Min
33.4   Typ
38   Max
13.1   Min
15.2   Typ
19   Max
15   Min
52   Typ
1.8   Typ
5.3   Typ
247   Typ
10.2   Typ
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106.
Physical Properties

No physical properties for this alloy

Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties
Technique Suitability
SolderingExcellent
BrazingExcellent
Oxyacetylene WeldingNot Recommended
Gas Shielded Arc WeldingNot Recommended
Coated Metal Arc WeldingNot Recommended
Spot WeldNot Recommended
Seam WeldNot Recommended
Butt WeldNot Recommended
Capacity for Being Cold WorkedPoor
Capacity for Being Hot FormedPoor
Machinability Rating84
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
PlumbingCu based devices for lead-free water applications,
Lead-free defined as Calif. AB 1953 max. .25% lead content
Lead-free, dezincification resistant for potable water components
valves, fittings, pumps, meters
Applicable Specifications
Form Sub-Form System Standard Description
As Sand CastASTMB584COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS
ValvesASTMB763/B763MCOPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS
IngotASTMB30COPPER BASE ALLOYS IN INGOT FORM
Corrosion Properties

No information available.