C89537
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | B | Bi | Mg | Si | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||||||||
| Min (%) | 84.0 | 3.0 | 5.0 | .0005 | .50 | .01 | .6 | ||
| Max (%) | 86.0 | .09 | 6.0 | 13.0 | .50 | .0020 | 3.0 | .10 | 1.2 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| As Sand Cast | As Sand Cast | M01 |
45 Typ |
21 Typ |
25 Typ |
| Melting Point - Liquidus°F | 1832 |
|---|---|
| Melting Point - Solidus°F | 1742 |
| Densitylb/cu in. at 68°F | 0.314 |
| Specific Gravity | 8.7 |
| Electrical Conductivity% IACS at 68°F | 15 |
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Plumbing | Lead-free defined by Calif. AB 1953, max .25% Pb content | ||
| Potable water valve bodies, faucets, plumbing components |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Sand Cast | ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS | ||
| Valves | ASTM | B763/B763M | COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS | ||
| Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties