Find suppliers for this alloy
C89540
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | Ni(2) | Al | Bi | Se | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
|||||||||
| Min (%) | 58.0 | 32.0 | 0.10 | 0.6 | |||||
| Max (%) | 64.0 | 0.10 | 1.2 | 38.0 | 0.50 | 1.0 | 0.60 | 1.2 | 0.10 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| As Sand Cast | As Sand Cast | M01 |
35 Min 48 Typ |
20 Min 28 Typ |
21 Min 29 Typ |
5 Min 8 Typ |
| Melting Point - Liquidus°F | 1638 |
|---|---|
| Melting Point - Solidus°F | 1588 |
Casting Characteristics
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Machinability Rating | 97 |
| Machinability Rating | 75 |
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Plumbing | Plumbing Castings | Lead Free | Lead Free |
| Plumbing Castings | Mechanical Properties | Moderate Strength |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Permanent Mold Cast | ASTM | B806 | PERMANENT MOLD CASTINGS | ||
| Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties