Find suppliers for this alloy
C89560
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | Al | B | Bi | Cd | |
|
(1) Cu + Sum of Named Elements 99.5% min. |
|||||||||
| Min (%) | 58.0 | 0.30 | 0.0003 | 1.0 | |||||
| Max (%) | 61.0 | 0.09 | 0.25 | Rem | 0.12 | 0.8 | 0.0015 | 2.4 | 0.001 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.2% Offset (ksi) |
Elongation (%) |
Vickers Hardness, 500 gm |
|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||
| Castings | As Pressure Die Cast | M04 |
51 Typ |
19 Typ |
5 Typ |
120 Typ |
| Melting Point - Liquidus°F | 1646 |
|---|---|
| Melting Point - Solidus°F | 1586 |
| Densitylb/cu in. at 68°F | 0.302 |
| Specific Gravity | 8.37 |
Casting Characteristics
| Technique | Suitability |
|---|---|
| Soldering | Good |
| Brazing | Good |
| Machinability Rating | 80 |
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties