Find suppliers for this alloyC89560
Chemical Composition
Element
Cu(1)PbSnZnFeAlBBiCd
(1) Cu + Sum of Named Elements 99.5% min.
Min (%)58.00.300.00031.0
Max (%)61.00.090.25Rem0.120.80.00152.40.001
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.2% Offset
Elongation
(%)
Vickers Hardness, 500 gm
CastingsAs Pressure Die CastM0451   Typ
19   Typ
5   Typ
120   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1646
Melting Point - Solidus°F1586
Densitylb/cu in. at 68°F0.302
Specific Gravity8.37
Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties
Technique Suitability
SolderingGood
BrazingGood
Machinability Rating80
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
IndustrialDie Castings
Applicable Specifications

No applicable specifications for this alloy

Corrosion Properties

No information available.