Find suppliers for this alloy
C89570
| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P | Ni(2) | Al | B | Bi | |
|
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co. |
||||||||||
| Min (%) | 58.0 | .20 | 35.0 | .05 | .15 | .10 | .0001 | .05 | ||
| Max (%) | 63.0 | .09 | 1.5 | 38.0 | .50 | .15 | .50 | 1.0 | .0020 | 1.5 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | |||||
| As Sand Cast | As Sand Cast | M01 |
50.8 Typ |
26.1 Typ |
15 Typ |
| Melting Point - Liquidus°F | 1688 |
|---|---|
| Melting Point - Solidus°F | 1652 |
| Densitylb/cu in. at 68°F | 0.303 |
| Specific Gravity | 8.4 |
| Electrical Conductivity% IACS at 68°F | 25 |
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Plumbing | Lead-free defined by Calif. AB 1953, max .25% Pb content | ||
| Potable water valve bodies, faucets, plumbing components | |||
| Valve Bodies, Faucets and Plumbing Componsnts |
| Form | Specific Sub-Form | Application | System | Standard | Description |
|---|---|---|---|---|---|
| As Sand Cast | Valves | ASTM | B763/B763M | COPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS | |
| ASTM | B584 | COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS | |||
| Ingot | ASTM | B30 | COPPER BASE ALLOYS IN INGOT FORM |
Corrosion Properties