Chemical Composition
Element
Cu(1)PbSnZnFePNi(2)AlBBi
(1) Cu + Sum of Named Elements 99.5% min. (2) Ni value includes Co.
Min (%)58.0.2035.0.05.15.10.0001.05
Max (%)63.0.091.538.0.50.15.501.0.00201.5
Mechanical Properties*
Form
Temper
Temper Code
Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
As Sand CastAs Sand CastM0150.8   Typ
26.1   Typ
15   Typ
* Measured at room temperature, 68°F (20°C).
Physical Properties
Melting Point - Liquidus°F1688
Melting Point - Solidus°F1652
Densitylb/cu in. at 68°F0.303
Specific Gravity8.4
Electrical Conductivity% IACS at 68°F25
Casting Characteristics

No casting characteristics for this alloy

Fabrication Properties
Technique Suitability
Machinability Rating90
Fabrication Process Properties

No fabrication process properties for this alloy

Thermal Characteristics

No thermal characteristics for this alloy

Typical uses
Product Category Product Reason Category Reason
PlumbingLead-free defined by Calif. AB 1953, max .25% Pb content
Potable water valve bodies, faucets, plumbing components
Valve Bodies, Faucets and Plumbing Componsnts
Applicable Specifications
Form Sub-Form System Standard Description
As Sand CastASTMB584COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS
ValvesASTMB763/B763MCOPPER ALLOY SAND CASTINGS FOR VALVE APPLICATIONS
IngotASTMB30COPPER BASE ALLOYS IN INGOT FORM
Corrosion Properties

No information available.