Find suppliers for this alloy
C90250
| Elements | ||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu | Pb | Sn | Zn | Fe | P | Ni | Al | Mn | S | Sb | Si | |
| Min (%) | 89.0 | 9.0 | ||||||||||
| Max (%) | 91.0 | 0.30 | 11.0 | 0.50 | 0.25 | 0.05 | 2.0 | 0.005 | 0.20 | 0.05 | 0.02 | 0.005 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties