Find suppliers for this alloyC90430
Chemical Composition
Element
Cu(1)PbSnZnFePNiBCMnSSbTiZr
(1) Cu + Sum of Named Elements 99.3% min.
Min (%)86.07.51.00.100.10
Max (%)89.00.098.55.00.400.051.00.100.100.200.651.50.100.10