Find suppliers for this alloy C92200
Chemical Composition
Elements
Cu(1,2) Pb Sn Zn Fe P(3) Ni(4) Al S Sb Si
(1) In determining Cu min., Cu may be calculated as Cu + Ni.
(2) Cu + Sum of Named Elements 99.3% min.
(3) For continuous castings P shall be 1.5% max.
(4) Ni value includes Co.
Min (%) 86.0 1.0 5.5 3.0
Max (%) 90.0 2.0 6.5 5.0 0.25 0.05 1.0 0.005 0.05 0.25 0.005
Mechanical Properties *
Form Temper Temper Code Tensile Strength
(ksi)
YS-0.5% Ext
(ksi)
Elongation
(%)
Brinell Hardness, 500 kg load Charpy V-Notch Impact Strength
(ft-lbs)
Compressive Strength .001 in. set/in.
(ksi)
Compressive Strength .01 in. set/in.
(ksi)
Compressive Strength .1 in. set/in.
(ksi)
Creep Strength (0.1% per 10,000 hours)
(ksi)
Fatigue Strength**
(ksi)
* Measured at room temperature, 68°F (20°C). ** Fatigue Strength: 100 x 106 cycles, unless indicated as [N] x 106.
As Centrifugal Cast As Centrifugal Cast M02 34 Min for Standard
34 Min for Standard
16 Min for Standard
22 Min for Standard
22 Min for Standard
As Continuous Cast As Continuous Cast M07 38 Min for Standard
38 Min for Standard
19 Min for Standard
18 Min for Standard
18 Min for Standard
As Permanent Mold Cast As Permanent Mold Cast M05 34 Min for Standard
16 Min for Standard
24 Min for Standard
As Sand Cast As Sand Cast M01 34 Min for Standard
34 Min for Standard
40 Typ
16 Min for Standard
20 Typ
22 Min for Standard
22 Min for Standard
30 Typ
65 Typ
19 Typ
15 Typ 20 Typ 38 Typ 11 Typ 11 Typ
Physical Properties
Melting Point - Liquidus°F 1810
Melting Point - Solidus°F 1518
Densitylb/cu in. at 68°F 0.312
Specific Gravity 8.64
Electrical Conductivity% IACS at 68°F 14
Thermal ConductivityBtu/ sq ft/ ft hr/ °F at 68°F 40.2
Coefficient of Thermal Expansion 68-57210 to -6 power per °F (68 – 572°F) 10
Specific Heat CapacityBtu/ lb /°F at 68°F 0.09
Modulus of Elasticity in Tensionksi 14000
Incipient Melting°F 600
Magnetic Permeability 1
Casting Characteristics
Casting Attribute Level
Casting Yield Medium
Drossing Low
Effect of Section Size High
Fluidity Medium
Gassing Medium
Patternmakers Shrinkage inches per inch 3/16
Shrinkage in Solidification Low
Fabrication Properties
Technique Suitability
Soldering Excellent
Brazing Excellent
Oxyacetylene Welding Not Recommended
Gas Shielded Arc Welding Not Recommended
Coated Metal Arc Welding Not Recommended
Machinability Rating 42
Common Fabrication Processes

No fabrication process properties for this alloy

Thermal Properties
Treatment Value* Time**
* Temperature is measured in Fahrenheit. ** Time is measured in minutes.
Stress Relief 500
Solution Treatment 0
Typical uses
Product Category Product Reason Category Reason
Architecture Ornamental Castings Corrosion Resistance Corrosion Resistance
Ornamental Castings Corrosion Resistance Corrosion Resistance to Numerous Environments
Ornamental Castings Machining Properties Machinability, Good
Ornamental Castings Mechanical Properties Moderate Strength
Building Cooling Equipment Conductivity (Thermal) Thermal Conductivity
Cooling Equipment Corrosion Resistance Corrosion Resistance
Cooling Equipment Corrosion Resistance Corrosion Resistance to Fresh Water
Cooling Equipment Corrosion Resistance Corrosion Resistance to Saline Solutions
Cooling Equipment Machining Properties Machinability, Good
Cooling Equipment Mechanical Properties Moderate Strength
Cooling Equipment Mechanical Properties Retains Strength at Elevated Temperatures
Cooling Equipment Pressure Tight Pressure Tight up to 260 C
Heating Equipment Conductivity (Thermal) Thermal Conductivity
Heating Equipment Corrosion Resistance Corrosion Resistance to Numerous Environments
Heating Equipment Machining Properties Machinability, Good
Heating Equipment Mechanical Properties Moderate Strength
Heating Equipment Mechanical Properties Retains Strength at Elevated Temperatures
Heating Equipment Pressure Tight Pressure Tight up to 260 C
Fasteners Nuts Corrosion Resistance Corrosion Resistance
Nuts Machining Properties Machinability, Good
Nuts Mechanical Properties Moderate Strength
Industrial Bearings Corrosion Resistance Corrosion Resistance
Bearings Corrosion Resistance Corrosion Resistance to Numerous Environments
Bearings Friction & Wear Properties Wear Resistance
Bearings Machining Properties Machinability, Good
Bearings Mechanical Properties Moderate Strength
Bushings Corrosion Resistance Corrosion Resistance
Bushings Friction & Wear Properties Wear Resistance
Bushings Machining Properties Machinability, Good
Bushings Mechanical Properties Moderate Strength
Cryogenic Valves Corrosion Resistance Corrosion Resistance
Cryogenic Valves Machining Properties Machinability, Good
Cryogenic Valves Mechanical Properties Moderate Strength
Cryogenic Valves Pressure Tight Pressure Tight up to 260 C
Fittings Used to 550 F Corrosion Resistance Corrosion Resistance
Fittings Used to 550 F Machining Properties Machinability, Good
Fittings Used to 550 F Mechanical Properties Moderate Strength
Fittings Used to 550 F Mechanical Properties Retains Strength at Elevated Temperatures
Gears Corrosion Resistance Corrosion Resistance
Gears Corrosion Resistance Corrosion Resistance to Fresh Water
Gears Corrosion Resistance Corrosion Resistance to Saline Solutions
Gears Friction & Wear Properties Wear Resistance
Gears Machining Properties Machinability, Good
Gears Mechanical Properties Moderate Strength
Medium Pressure Hydraulic Equipment Corrosion Resistance Corrosion Resistance
Medium Pressure Hydraulic Equipment Corrosion Resistance Corrosion Resistance to Numerous Environments
Medium Pressure Hydraulic Equipment Machining Properties Machinability, Good
Medium Pressure Hydraulic Equipment Mechanical Properties Moderate Strength
Medium Pressure Hydraulic Equipment Mechanical Properties Retains Strength at Elevated Temperatures
Medium Pressure Hydraulic Equipment Pressure Tight Pressure Tight up to 260 C
Piston Rings Corrosion Resistance Corrosion Resistance
Piston Rings Corrosion Resistance Corrosion Resistance to Numerous Environments
Piston Rings Machining Properties Machinability, Good
Piston Rings Mechanical Properties Moderate Strength
Piston Rings Pressure Tight Pressure Tight up to 260 C
Pump Impellers Corrosion Resistance Corrosion Resistance (Excellent)
Pump Impellers Machining Properties Machinability, Good
Pump Impellers Mechanical Properties Moderate Strength
Pumps Used to 550 F Corrosion Resistance Corrosion Resistance
Pumps Used to 550 F Corrosion Resistance Corrosion Resistance to Fresh Water
Pumps Used to 550 F Corrosion Resistance Resistant in Saline Solutions
Pumps Used to 550 F Friction & Wear Properties Wear Resistance
Pumps Used to 550 F Machining Properties Machinability, Good
Pumps Used to 550 F Mechanical Properties Moderate Strength
Pumps Used to 550 F Mechanical Properties Retains Strength at Elevated Temperatures
Valve Components Corrosion Resistance Corrosion Resistance
Valve Components Corrosion Resistance Corrosion Resistance to Fresh Water
Valve Components Corrosion Resistance Resistant in Saline Solutions
Valve Components Friction & Wear Properties Wear Resistance
Valve Components Machining Properties Machinability, Good
Valve Components Mechanical Properties Moderate Strength
Valves for Water Meters Corrosion Resistance Corrosion Resistance
Valves for Water Meters Corrosion Resistance Corrosion Resistance to Fresh Water
Valves for Water Meters Corrosion Resistance Resistant in Saline Solutions
Valves for Water Meters Friction & Wear Properties Wear Resistance
Valves for Water Meters Machining Properties Machinability, Good
Valves for Water Meters Mechanical Properties Moderate Strength
Marine Marine Castings Corrosion Resistance Corrosion Resistance
Marine Castings Corrosion Resistance Corrosion Resistance to Fresh Water
Marine Castings Corrosion Resistance Corrosion Resistance to Numerous Environments
Marine Castings Corrosion Resistance Corrosion Resistance to Saline Solutions
Marine Castings Machining Properties Machinability, Good
Marine Castings Mechanical Properties Moderate Strength
Plumbing Medium Pressure Steam Equipment to 550 F Corrosion Resistance Corrosion Resistance
Medium Pressure Steam Equipment to 550 F Corrosion Resistance Corrosion Resistance to Numerous Environments
Medium Pressure Steam Equipment to 550 F Machining Properties Machinability, Good
Medium Pressure Steam Equipment to 550 F Mechanical Properties Moderate Strength
Medium Pressure Steam Equipment to 550 F Mechanical Properties Retains Strength at Elevated Temperatures
Medium Pressure Steam Equipment to 550 F Pressure Tight Pressure Tight to 260 C
Applicable Specifications
Form Specific Sub-Form Application System Standard Description
As Centrifugal Cast Castings ASTM B271/B271M COPPER BASE ALLOY CENTRIFUGAL CASTINGS
Castings SAE J461 WROUGHT AND CAST COPPER ALLOYS
Castings SAE J462 CAST COPPER ALLOYS
As Continuous Cast Castings SAE J462 CAST COPPER ALLOYS
Castings SAE J461 WROUGHT AND CAST COPPER ALLOYS
Castings ASTM B505/B505M COPPER BASE ALLOY CONTINUOUS CASTINGS
As Sand Cast Castings SAE J462 CAST COPPER ALLOYS
Castings SAE J461 WROUGHT AND CAST COPPER ALLOYS
Castings ASTM B584 COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS
Castings ASTM B61 STEAM OR VALVE BRONZE CASTINGS
Castings ASME SB584 COPPER ALLOY SAND CASTINGS FOR GENERAL APPLICATIONS
Castings ASME SB61 STEAM OR VALVE BRONZE CASTINGS
Fitting ASME SB61 STEAM OR VALVE BRONZE CASTINGS
ASTM B61 STEAM OR VALVE BRONZE CASTINGS
FEDERAL WW-P-460 PIPE FITTINGS: BRASS OR BRONZE
ASME B16.24 BRONZE PIPE FLANGES AND FLANGED FITTINGS
Flanges ASTM B61 STEAM OR VALVE BRONZE CASTINGS
ASME SB61 STEAM OR VALVE BRONZE CASTINGS
FEDERAL WW-P-460 PIPE FITTINGS: BRASS OR BRONZE
Ingot
ASTM B30 COPPER BASE ALLOYS IN INGOT FORM
Valves
MILITARY MIL-V-17547 VALVE, CHECK, BRONZE
Corrosion Properties

No Corrosion Properties Available.