C92220
| Elements | |||||||
|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P(2) | Ni(3) | |
|
(1) In determining Cu min., Cu may be calculated as Cu + Ni. (2) For continuous castings P shall be 1.5% max. (3) Ni value includes Co. |
|||||||
| Min (%) | 86.0 | 1.5 | 5.0 | 3.0 | 0.50 | ||
| Max (%) | 88.0 | 2.5 | 6.0 | 5.5 | 0.25 | 0.05 | 1.0 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties