C92310
| Elements | ||||||||
|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Ni(3) | Al | Mn | Si | |
|
(1) Cu + Sum of Named Elements 99.3% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) Ni value includes Co. |
||||||||
| Min (%) | 0.30 | 7.5 | 3.5 | |||||
| Max (%) | Rem | 1.5 | 8.5 | 4.5 | 1.0 | 0.005 | 0.03 | 0.005 |