| Elements | ||||||||||
|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Al | Mn | Sb | Si | |
|
(1) In determining Cu min., Cu may be calculated as Cu + Ni. (2) Cu + Sum of Named Elements 99.3% min. (3) Ni value includes Co. |
||||||||||
| Min (%) | 2.5 | 6.0 | 1.5 | |||||||
| Max (%) | Rem | 3.5 | 8.0 | 3.0 | 0.20 | 0.20 | 0.005 | 0.05 | 0.25 | 0.005 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties