C92600
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1) | Pb | Sn | Zn | Fe | P(2) | Ni(3) | Al | S | Sb | Si | |
|
(1) In determining Cu min., Cu may be calculated as Cu + Ni. (2) For continuous castings P shall be 1.5% max. (3) Ni value includes Co. |
|||||||||||
| Min (%) | 86.0 | 0.8 | 9.3 | 1.3 | |||||||
| Max (%) | 88.5 | 1.5 | 10.5 | 2.5 | 0.20 | 0.03 | 0.7 | 0.005 | 0.05 | 0.25 | 0.005 |
| Form | Temper | Temper Code | Tensile Strength (ksi) |
YS-0.5% Ext (ksi) |
Elongation (%) |
Rockwell F scale | Brinell Hardness, 500 kg load | Izod (ft-lbs) |
Compressive Strength .001 in. set/in. (ksi) |
Compressive Strength .1 in. set/in. (ksi) |
|---|---|---|---|---|---|---|---|---|---|---|
| * Measured at room temperature, 68°F (20°C). | ||||||||||
| As Sand Cast | As Sand Cast | M01 |
40 Min for Standard 44 Typ |
18 Min for Standard 20 Typ |
20 Min for Standard 30 Typ |
78 Typ |
70 Typ |
7 Typ | 12 Typ | 40 Typ |
| Melting Point - Liquidus°F | 1800 |
|---|---|
| Melting Point - Solidus°F | 1550 |
| Densitylb/cu in. at 68°F | 0.315 |
| Specific Gravity | 8.72 |
| Electrical Conductivity% IACS at 68°F | 9 |
| Coefficient of Thermal Expansion 68-39210 to -6 power per °F (68 – 392°F) | 10 |
| Specific Heat CapacityBtu/ lb /°F at 68°F | 0.09 |
| Modulus of Elasticity in Tensionksi | 15000 |
| Casting Attribute | Level |
|---|---|
| Casting Yield | Medium |
| Drossing | Low |
| Effect of Section Size | High |
| Fluidity | Medium |
| Gassing | Medium |
| Patternmakers Shrinkage inches per inch | 3/16 |
| Shrinkage in Solidification | Low |
| Technique | Suitability |
|---|---|
| Soldering | Excellent |
| Brazing | Good |
| Oxyacetylene Welding | Not Recommended |
| Gas Shielded Arc Welding | Not Recommended |
| Coated Metal Arc Welding | Not Recommended |
| Machinability Rating | 40 |
Common Fabrication Processes
| Treatment | Value* | Time** | ||
|---|---|---|---|---|
| * Temperature is measured in Fahrenheit. ** Time is measured in minutes. | ||||
| Stress Relief | 500 | |||
| Solution Treatment | 0 | |||
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Fasteners | Lead Screw Nuts | Corrosion Resistance | Corrosion Resistance |
| Lead Screw Nuts | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Lead Screw Nuts | Machining Properties | Machinability, Good | |
| Lead Screw Nuts | Mechanical Properties | Moderate Strength | |
| Nuts | Corrosion Resistance | Corrosion Resistance | |
| Nuts | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Nuts | Machining Properties | Machinability, Good | |
| Nuts | Mechanical Properties | Moderate Strength | |
| Industrial | Bushings | Corrosion Resistance | Corrosion Resistance |
| Bushings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Bushings | Friction & Wear Properties | Wear Resistance | |
| Bushings | Machining Properties | Machinability, Good | |
| Bushings | Mechanical Properties | Moderate Strength | |
| Fittings | Corrosion Resistance | Corrosion Resistance | |
| Fittings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Fittings | Machining Properties | Machinability, Good | |
| Fittings | Mechanical Properties | Moderate Strength | |
| Gears | Corrosion Resistance | Corrosion Resistance | |
| Gears | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Gears | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Gears | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
| Gears | Machining Properties | Machinability, Good | |
| Gears | Mechanical Properties | Moderate Strength | |
| Heavy Duty Bearings | Corrosion Resistance | Corrosion Resistance | |
| Heavy Duty Bearings | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Heavy Duty Bearings | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
| Heavy Duty Bearings | Friction & Wear Properties | Wear Resistance | |
| Heavy Duty Bearings | Machining Properties | Machinability, Good | |
| Heavy Duty Bearings | Mechanical Properties | Moderate Strength | |
| Piston Rings | Corrosion Resistance | Corrosion Resistance | |
| Piston Rings | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Piston Rings | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
| Piston Rings | Friction & Wear Properties | Wear Resistance | |
| Piston Rings | Machining Properties | Machinability, Good | |
| Piston Rings | Mechanical Properties | Moderate Strength | |
| Piston Rings | Pressure Tight | Pressure Tight below 260 C | |
| Pump Impellers | Corrosion Resistance | Corrosion Resistance | |
| Pump Impellers | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Pump Impellers | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Pump Impellers | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
| Pump Impellers | Friction & Wear Properties | Wear Resistance | |
| Pump Impellers | Machining Properties | Machinability, Good | |
| Pump Impellers | Mechanical Properties | Moderate Strength | |
| Pump Pistons | Corrosion Resistance | Corrosion Resistance | |
| Pump Pistons | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Pump Pistons | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Pump Pistons | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
| Pump Pistons | Friction & Wear Properties | Wear Resistance | |
| Pump Pistons | Machining Properties | Machinability, Good | |
| Pump Pistons | Mechanical Properties | Moderate Strength | |
| Steam Castings | Corrosion Resistance | Corrosion Resistance | |
| Steam Castings | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Steam Castings | Friction & Wear Properties | Wear Resistance | |
| Steam Castings | Machining Properties | Machinability, Good | |
| Steam Castings | Mechanical Properties | Moderate Strength | |
| Steam Castings | Pressure Tight | Pressure Tight below 260 C | |
| Valve Bodies | Corrosion Resistance | Corrosion Resistance | |
| Valve Bodies | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Valve Bodies | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Valve Bodies | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
| Valve Bodies | Machining Properties | Machinability, Good | |
| Valve Bodies | Mechanical Properties | Moderate Strength | |
| Valves | Corrosion Resistance | Corrosion Resistance | |
| Valves | Corrosion Resistance | Corrosion Resistance to Fresh Water | |
| Valves | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Valves | Corrosion Resistance | Corrosion Resistance to Saline Solutions | |
| Valves | Friction & Wear Properties | Wear Resistance | |
| Valves | Machining Properties | Machinability, Good | |
| Valves | Mechanical Properties | Moderate Strength |