Find suppliers for this alloy
C92610
| Elements | |||||||||
|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | Ni(3) | Al | Mn | Si | |
|
(1) In determining Cu min., Cu may be calculated as Cu + Ni. (2) Cu + Sum of Named Elements 99.3% min. (3) Ni value includes Co. |
|||||||||
| Min (%) | 0.30 | 9.5 | 1.7 | ||||||
| Max (%) | Rem | 1.5 | 10.5 | 2.8 | 0.15 | 1.0 | 0.005 | 0.03 | 0.005 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties