Find suppliers for this alloy
C92710
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P(3) | Ni(4) | Al | S | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.3% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) For continuous castings P shall be 1.5% max. (4) Ni value includes Co. |
|||||||||||
| Min (%) | 4.0 | 9.0 | |||||||||
| Max (%) | Rem | 6.0 | 11.0 | 1.0 | 0.20 | 0.10 | 2.0 | 0.005 | 0.05 | 0.25 | 0.005 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
Typical Uses
Applicable Specifications
Corrosion Properties