Find suppliers for this alloy
C93100
| Elements | |||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|
| Cu(1,2) | Pb | Sn | Zn | Fe | P(3) | Ni(4) | Al | S | Sb | Si | |
|
(1) Cu + Sum of Named Elements 99.0% min. (2) In determining Cu min., Cu may be calculated as Cu + Ni. (3) For continuous castings P shall be 1.5% max. (4) Ni value includes Co. |
|||||||||||
| Min (%) | 2.0 | 6.5 | |||||||||
| Max (%) | Rem | 5.0 | 8.5 | 2.0 | 0.25 | 0.30 | 1.0 | 0.005 | 0.05 | 0.25 | 0.005 |
Mechanical Properties
Physical Properties
Casting Characteristics
Fabrication Properties
Common Fabrication Processes
Thermal Properties
| Product Category | Product | Reason Category | Reason |
|---|---|---|---|
| Electrical | Electrical Parts Requiring Moderate Strength | Conductivity (Electrical) | Electrical Conductivity |
| Electrical Parts Requiring Moderate Strength | Conductivity (Thermal) | Thermal Conductivity | |
| Electrical Parts Requiring Moderate Strength | Corrosion Resistance | Corrosion Resistance | |
| Electrical Parts Requiring Moderate Strength | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Electrical Parts Requiring Moderate Strength | Mechanical Properties | Moderate Strength | |
| Industrial | Thermal Conductors Requiring Moderate Strength | Conductivity (Thermal) | Thermal Conductivity |
| Thermal Conductors Requiring Moderate Strength | Corrosion Resistance | Corrosion Resistance | |
| Thermal Conductors Requiring Moderate Strength | Corrosion Resistance | Corrosion Resistance to Numerous Environments | |
| Thermal Conductors Requiring Moderate Strength | Mechanical Properties | Moderate Strength |
Applicable Specifications
Corrosion Properties